摘要
广西合浦地区高铁低品级高岭土由于铁含量高,原矿Fe2O3+TiO2>2.5%,经淘洗后获得的-0.045mm粒级样品中的铁含量大于4%。通过试验研究表明,采用高梯度磁选、加温漂白等方法,可获得Al2O3>35%,Fe2O3<1.5%,白度大于80%的漂白精土产品。
Because high-iron and low-grade kaolin in Hepu Guangxi is a high iron content, in the ore Fe203+TiO2〉2.5%. After washing, in -0.045ram size fraction of the iron content of greater than 4%. Research shows that, by high gradient magnetic separation, heating bleaching methods can be obtained A1203〉35%, Fe203〈1.5%, greater than 80% of whiteness bleaching products.
出处
《中国非金属矿工业导刊》
2012年第1期20-23,共4页
China Non-Metallic Minerals industry
基金
广西自然科学基金项目(桂科自0991062)
关键词
高铁低品级高岭土
高梯度磁选
漂白
除铁
广西合浦
high-iron and low-grade kaoline
high-gradient magnetic separation
bleach
iron removal
Hepu Guangxi