蒸汽直接加热模腔的高光注塑技术研究 被引量:4

RESEARCH OF HIGH-GLOSS INJECTION TECHNOLOGY WITH DIRECT STEAM HEATING THE MOLD CAVITY
下载PDF
导出
摘要 提出了蒸汽直接加热模具型腔表面的高光注塑新方法,研制了蒸汽直接加热模具型腔的高光注塑模具及模具温度控制机。该装置将高温蒸汽直接通入模腔,使模腔表面达到所需的温度,然后通入高温干空气,吹除模腔内残留的冷凝水,再注射、保压、冷却、开模,完成一个注塑周期。该方法使动定模模面得到均匀加热,熔融料前锋温度和速度高,且只加热模面以下1~2 mm的模芯,能有效地缩短加热和冷却时间。结果表明,该技术能够有效地解决塑料件的熔接痕、流痕、翘曲、缩水、尺寸变形等缺陷,使塑料件获得极高的表面粗糙度等级,且节省热能,降低相关的模具制造成本。 A novel high-gloss injection method which the mold cavity was heated by steam directly was presented,the related high-gloss mold and special high-gloss mold temperature controller was developed.By this machine,the high-temperature steam was input the mold cavity for several seconds and the surface of mold cavity gained the demandable temperature,then the high-temperature dry air was switched to the mold cavity for blowing off residual condensation water on the surface of mold cavity.Subsequently,a cycle of injection molding was completed,including injection,packing,cooling,and mold opening.Surface of fixed and moving half molds were heated evenly by this method,the speed and temperature of the front of molten plastic were very high,and the metal of mold cores with depth of only 1–2?mm from mold surfaces was heated,so the method greatly shortened the heating and cooling time.The experimental results showed that the surface defects of plastic parts were improved effctively such as welding mark,flow mark,warping,craters,size deformation,et al.And extreme high grade of surface roughness was obtained,the technology also reduced heat energy consumption and saved mold manufacturing costs.
出处 《工程塑料应用》 CAS CSCD 北大核心 2011年第12期35-38,共4页 Engineering Plastics Application
基金 国家自然科学基金项目(60978039)
关键词 蒸汽直接加热模腔 高光注塑模具 高光模温机 注塑工艺 direct steam heating mold cavity high-gloss injection mold high-gloss mold temperature controller injection technology
  • 相关文献

参考文献5

二级参考文献42

共引文献67

同被引文献21

  • 1赵永成,吴亚南,董淑婧.注塑成型收缩率影响因素的分析[J].塑料工业,2005,33(12):29-31. 被引量:27
  • 2朱利平.塑料阀门在工业管道中的要求与应用[J].化工设备与管道,2006,43(2):57-61. 被引量:3
  • 3Chang R Y, Tsaur B D. Experimental and theoretic studies of shrinkage, warpage, and sink marks of crystalline polymer injection molded parts E J ]. Polymer Engineering and Science, 1995,35 ( 15 ): 1 222-1 230. 被引量:1
  • 4Jansen K M B, Van Dijk D J, Husselman M H. Effect of processing conditions on shrinkage in injection-molding E J ]. Polymer Engineering and Science, 1998,38 ( 5 ) : 838-846. 被引量:1
  • 5黄虹宾,杨继跃.一种球阀阀体和球阀密封圈固定座的定位机构:中国,CN201568599[P].2010-09-01. 被引量:1
  • 6齐斌.光盘盘基精密注塑压缩成型模具的设计与研究[D].青岛:青岛科技大学.2008. 被引量:1
  • 7深圳市莱奥德机械有限公司,标准油温机产品介绍[EB/OL].(2014-06-18)[2014-08-15].http://www.gaszjx-ad.com/pro18.html. 被引量:1
  • 8北京利德盛机械有限公司,蒸汽传热的蒸汽模温机产品介绍[EB/OL].(2014-05-16)[2014-07-27].http://www.gtobal.com/selFdetail-1671874302.html. 被引量:1
  • 9KILWON C,SUNGHEE A, JINBAE P, et al. Evaluation of the weld- line strength of thermoplastics by compact tension test[J]. Polym Eng Sc,i 2013,37(7) :1 217 - 1 225. 被引量:1
  • 10JKLHo, KPChu, CKMOK. Minimizing manufacturinge costsfor thin injection molded Plastieeomv compontens [ J]. Int J Adv Manuf Technol,2014,8 (12) : 159 - 190. 被引量:1

引证文献4

二级引证文献12

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部