期刊文献+

15CrMoR+00Cr17Ni14Mo2/N08825复合板洗涤塔制造工艺择议 被引量:4

Discussion on Fabrication Procedure for Scrubbing Tower Using Clad Steel Plate 15CrMoR+00Cr17Ni14Mo2/N08825
下载PDF
导出
摘要 以某洗涤塔制造为例,针对技术条件要求爆炸复合的15CrMoR+00Cr17Ni14M02不锈钢复合钢板和15CrMoR+N08825(0Cr21Ni42M03Cu2Ti)镍合金复合钢板冷成形后采取正火加回火工艺只能恢复基材的供货状态,而由此导致在σ相析出温度(600~950℃)和敏化温度(300~840℃)长时间停留会破坏覆层耐蚀性的实际情况,通过对其供货状态、设备制造过程的成形、焊接和热处理工艺综合分析,制定了合理的热成形和热处理工艺,保证了产品基层材料的使用状态为正火加回火状态,覆层使用状态分别为固溶或退火状态,产品各项性能均满足设计要求。 Using scrubbing tower as an example, aiming at the technical specification the supply condition of normalization plus tempering after cold formation for the clad of stainless steel and the nickel alloy cladding steel plate was seriously required, while the anti corrosion would be destructed at σ exudation temperature (600~950℃) and sensitive temperature (300~840℃). The analysis on such clad plate supply condition, forming, welding and heat treatment was made to set up an ideal forming and heat treatment processing and the base material was insured to use normalization plus temper heat treatment and the clad solution treatment. The performances of the product conform to design requirement.
出处 《石油化工设备》 CAS 2011年第5期61-65,共5页 Petro-Chemical Equipment
关键词 洗涤塔 不锈钢复合钢板 镍合金复合钢板 成形 焊接 热处理 scrubbing tower stainless clad plate nickel alloy clad steel plate forming heat treating
  • 相关文献

参考文献20

  • 1JB/T 4710-2005,钢制塔式容器[S]. 被引量:71
  • 2JB/T4759-2006,镍及镍合金压力容器[s]. 被引量:1
  • 3JB4733-1996.压力容器用爆炸不锈钢复合钢板[S].[S].,.. 被引量:9
  • 4JB4748-2002,压力容器用镍及镍合金爆炸复合钢板[S]. 被引量:1
  • 5郑远谋,张胜军.不锈钢-钢爆炸复合板结合区的电子探针研究[J].电子显微学报,1999,18(4):468-473. 被引量:6
  • 6刘俞铭.不锈钢、不锈钢制品表面处理与焊接新技术新工艺及钢号中外对照速查手册[M].北京:学苑出版社,2008. 被引量:1
  • 7GB/T21433-2008,不锈钢压力容器晶间腐蚀敏感性检验[s]. 被引量:7
  • 8GB/T4237-2007,不锈钢热轧钢板和钢带[S]. 被引量:17
  • 9GB6654-1996.压力容器用钢板[S].[S].中华人民共和国冶金工业部,.. 被引量:27
  • 10王富岗,王焕庭主编..石油化工高温装置材料及其损伤[M].大连:大连理工大学出版社,1991:157.

二级参考文献43

共引文献816

同被引文献34

引证文献4

二级引证文献10

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部