累积法预测在役管道腐蚀极限厚度计算方法

Cumulative-sum method to predict the corrosion limit thickness of in-service pipeline
原文传递
导出
摘要 为了方便、准确地确定腐蚀缺陷对在役管道剩余强度和承压能力的影响,基于含缺陷管道的弹性极限准则,应用ANSYS有限元软件分别对两种缺陷模型进行模拟分析,得到了不同缺陷尺寸条件下腐蚀区域的Mises应力。利用有限元分析结果,同时考虑腐蚀缺陷长度、宽度及深度等几何尺寸因素的影响,采用累积法确定在役腐蚀管道的Mises应力与腐蚀缺陷尺寸的函数关系。基于累积法确定的Mises应力公式,采用VisualBasic语言编制了在役管道腐蚀极限厚度计算软件,为工程技术人员在实际工程中的使用提供了计算工具和方法。 In order to determine the influence of corrosion defect on the residual strength and bearing capacity of in-service pipeline conveniently and accurately,finite element software ANSYS is applied to simulate two kinds of defect models,which is based on the elastic limit guidelines of pipeline with defects,and gets the Mises stresses of corrosion area under different defect sizes.According to the calculation results and considering the corrosion defect influences such as length,width and depth,cumulative-sum method is used to determine the function between Mises stress and defect size.Calculating software for pipeline corrosion limit thickness is developed by Visual Basic,which provides a convenient calculating tool to engineers in practical projects.
出处 《油气储运》 CAS 北大核心 2011年第8期643-646,592,共4页 Oil & Gas Storage and Transportation
关键词 在役管道 累积法 腐蚀极限厚度 缺陷模型 Mises应力 预测 in-service pipeline,cumulative-sum method,corrosion limit thickness,defect model,Mises stress
  • 相关文献

参考文献9

二级参考文献34

  • 1帅健,张春娥,陈福来.基于爆破试验数据对腐蚀管道剩余强度评定方法的验证[J].压力容器,2006,23(10):5-8. 被引量:20
  • 2帅健,张春娥,陈福来.腐蚀管道剩余强度评价方法的对比研究[J].天然气工业,2006,26(11):122-125. 被引量:88
  • 3Wang Y S. A plastic limit criterion for the remaining strength of corroded pipe: Proceedings of the International Conference on Offshore Mechanics and Arctic Engineering (10th), Stavanger, Norway,June 23-28,1991[C]. Stavanger:ASME, 1991. 被引量:1
  • 4Hopkins P,Jones D G. A study of the behavior of long and complex-shape corroded in transmission pipelines:Proceedings of the 1 lth International Conference of Mechanic and Arctic Engineering, Calgary, Canada, June 7-11,1992[C]. Calgary : ASME, 1992. 被引量:1
  • 5Fu Bin. Advanced methods for integrity assessment on corroded pipelines: Proceedings of 1996 Pipeline Reliability Conference, Houston, USA, Nov. 19-22,1996[C]. Houston : ASME, 1996. 被引量:1
  • 6Cronin D S, Andrew R K, Pick R J. Assessment of long corrosion grooves in line pipe:Proceedings of the 1st International Pipeline Conference, Calgary, Canada, June 9- 14, 1996[C]. Calgary: ASME,1996 被引量:1
  • 7Chouchaoui B A, Pick R J, Yost D B. Burst pressure predictions of line pipe containing single corrosion pits using the finite element method: Proceedings of the l lth International Conference of Offshore Mechanic and Arctic Engingeering,Calgary,Canada, June 7-11,1992[C]. Calgary : ASME, 1992. 被引量:1
  • 8Chouehaoui B A,Pick R J. Behavior of circumferentially aligned corrosion pits [J]. International Journal of Pressure Vessels and Piping, 1994,2(57) :187-200. 被引量:1
  • 9Bjornoy O H,Sigurdsson G,Cramer E H. Residual burst strength of corroded pipelines.-Proceedings of the 10th International Off shore and Polar Engineering Conference, Seattle, USA, May 28 June 2,2000[C]. Seattle : ASME, 2000. 被引量:1
  • 10Adilson C,Benjamin R D,Jose Luis F,et al. Burst tests on pipeline with long external corrosion:Proceedings of the 3rd Interna tional Pipeline Conference, Calgary, Canada, Oct. 1 - 5,2000 [ C] Calgary: ASME, 2000. 被引量:1

共引文献145

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部