对HOY生产的关键技术做了简要论述。生产HOY的原料质量要求较高,干切片含水率应控制在20μg/g以下,HOY的纺丝温度。
The technological key of HOY production was briefly discussed. HOY production requires higher\|quality chips. The water pick\|up of dried chips should be controlled below 20 g/g. The process parameters such as spinning temperature, quenching temperature and collection position etc. play important roles in the production.