摘要 In recent times, silicone rubber insulating material is used for power transmission line and substation insulation applications. In the present work, tracking and erosion resistance of the micro size filled and nano size filled silicone rubber material has been studied under the AC voltage, with ammonium chloride as a contaminant, as per IEC 60587 test procedures. The characteristic changes in the tracking resistance of the micro size and nano size filled specimens are analyzed through leakage current measurement. Comparative Tracking Index (CTI) is also evaluated in order to understand the relative behavior of solid electrical insulating material with regard to their susceptibility to surface tracking. Trend followed by the fundamental, third harmonic and fifth harmonic components of the leakage current during the tracking study are analyzed using moving average current technique. It is observed that the harmonic components of leakage current show good correlation with the tracking and erosion resistance of the material. It is noticed that 5 % wt ofnano size filler gives similar performance to that of 30 % wt of micro size filler in silicone composites.
机构地区 SonaPERT R&D Centre
出处 《Journal of Energy and Power Engineering》 2010年第9期32-40,共9页 能源与动力工程(美国大卫英文)
关键词 Outdoor insulator silicone rubber tracking resistance leakage current nano filler third harmonic 高压绝缘 复合材料 跟踪性 侵蚀性 纳米硅 泄漏电流测量 电绝缘材料 硅橡胶材料
  • 相关文献

参考文献8

  • 1R.S. Gorur, E.A. Chemey, J.T. Bumham, Outdoor Insulators, Ravi S. Gorur, Inc., Phoenix, Arizona, USA, 1999. 被引量:1
  • 2L.H. Meyer, Tracking and erosion resistance of RTV silicone rubber: effect of filler particle size and loading, IEEUPES Transmission & Distribution Conference & Exposition, Latin America, 2004, pp.453-456. 被引量:1
  • 3L.H. Meyer, E.A. Cherney, S.H. Jayaram, The role of inorganic fillers in silicone rubber for outdoor insulation-alumina tri-hydrate or silica, IEEE Electrical Insulation Magazine 20 (4) (2004) 13-21. 被引量:1
  • 4A.H. El-Hag, L.C. Simon, S.H. Jayaram, E.A. Cherney, Erosion resistance of nano filled silicone rubber, IEEE Transactions on Dielectrics and Electrical Insulation 13 (1) (2006) 122-128. 被引量:1
  • 5IEC publication 60-587- Testing method for evaluating the resistance of tracking and erosion of electrical insulating materials used under severe ambient conditions, 1984. 被引量:1
  • 6R. Sarathi, S. Chandrasekar, N. Yoshimura, Investigations into the surface condition of the silicone rubber insulation material using multiresolution signal decomposition, IEEE Transactions on Power Delivery 21 (1) (2006) 243-252. 被引量:1
  • 7S. Chandrasekar, S. Prabhu, K. Krishnamoorthi, R. Sarathi, Analysis of surface condition of polymeric insulation structure using wavelet packet transform, in: Proceedings of International conference on Power systems (ICPS'07), CPRI, Bangalore, Dec 2007. 被引量:1
  • 8S. Chandrasekar, S. Prabhu, S. Karthikeyan, K. Satheesh Kumar, R. Sarathi, Analysis of surface tracking of outdoor polymeric insulators using S-transform, in: National Conference on Electrical engineering and Embedded Systems, NCEE'08, College of Engineering Guindy, Anna University, Chennai, 20-21 Mar. 2008, pp. 175-179. 被引量:1