摘要
目的:比较镍铬合金烤瓷冠和钴铬合金烤瓷冠对牙龈组织的影响。方法:对100例单个后牙金属烤瓷冠修复患者分别制作镍铬合金、钴铬合金烤瓷冠各50件,1年后以牙龈指数为标准,评价牙龈健康状况。结果:牙龈健康状况:钴铬合金烤瓷冠A40例、B8例、C2例、D0例;镍铬合金烤瓷冠A28例、B10例、C7例、D5例。两者比较,差异有统计学意义(χ2=10.118,P=0.018)。结论:钴铬合金对牙龈组织的不利影响较镍铬合金轻。
Objective:To compare the effect of Co-Cr and Ni-Cr PFM to gingiva.Methods:100 cases of patients who needed to restore single molars were divided into two groups,and were respectively made 50 pieces of Co-Cr and Ni-Cr PFM.After one year,the state of gingiva were evaluated as the principle of gingival index.Results:The state of gingiva was Co-Cr alloy:A 40,B 8,C 2,D 0 and Ni-Cr alloy:A 28,B 10,C 7,D 5,there was a significant difference between the two groups (χ2=10.118,P=0.018).Conclusion:The adverse influence of Co-Cr PFM to gingiva is lighter than Ni-Cr.
出处
《中国医药导报》
CAS
2010年第3期32-32,34,共2页
China Medical Herald
关键词
钴铬合金
镍铬合金
牙龈指数
Cobalt-chromium
Nickel-chromium
Gingival index