核岛反应堆主回路奥氏体不锈钢大口径厚壁管道的焊接是核电站安装工程中的关键,而该管道焊接质量的控制,更是核电站建设质量控制的关键。本文就岭澳核电站二期3#机组主回路管道的焊接质量控制作一介绍,希望对以后核电站反应堆主回路管道的焊接质量控制能起到一定的借鉴作用。
In the nuclear power station construction, the key of the erection works of nuclear power station was the welding of the nuclear reactor primary loop made of austenitic stainless steel pipe with big diameter and thick wall. The welding quality played an important role in the quality control of the nuclear power station construction. The welding quality control of the primary loop pipe in the 3# unit of Lingao nuclear power station-Ⅱ was introduced in this paper. Expect to use for reference for welding quality control of primary loop pipe in the nuclear reactor pile here after.