摘要 Bi system tapes were prepared using the powder in tube method. The tapes were processed to their final thickness by repeated rolling and pressing and by a combination of rolling and pressing with intermediate heat treatment. The different processing techniques greatly affected the critical current density J c of the tapes because the homogeneity of the ceramic core and the propensity for crack formation within the tapes mainly depended on the deformation process. Bi system tapes were prepared using the powder in tube method. The tapes were processed to their final thickness by repeated rolling and pressing and by a combination of rolling and pressing with intermediate heat treatment. The different processing techniques greatly affected the critical current density J c of the tapes because the homogeneity of the ceramic core and the propensity for crack formation within the tapes mainly depended on the deformation process.
出处 《Tsinghua Science and Technology》 SCIE EI CAS 1998年第2期76-79,共4页 清华大学学报(自然科学版(英文版)
关键词 superconducting tapes critical current density PROCESSING superconducting tapes critical current density processing
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部