摘要 考察了贫化温度、硫化剂、还原剂、缓冷速率等因素对炼铜水淬渣中铜回收指标的影响。试验表明,当贫化温度保持在1350℃、硫化剂黄铁矿配比为5%、还原剂煤粉与硫化剂之比为1∶4、缓冷速率为5K/m in时,可获得粗选铜回收率78%左右、粗选精矿铜品位5.8%左右的技术指标。 The factors influencing copper recovery, such as impoverishment temperature, curing ingredient, reductant and the velocity of slow cooling were studied. The results indicated that the optimal impoverishment-flotation efficiency was obtained when the impoverishment temperature is kept at 1350℃,the dosage of the iron pyrite is 5%,the mixture ratio of the reductant coal fines and curing ingredient is 1 : 4, and the velocity of slow cooling is 5K/min. A concentrate of 5.8% copper content and a copper recovery of 78% is produced.
出处 《矿产综合利用》 CAS 2009年第2期37-40,共4页 Multipurpose Utilization of Mineral Resources
关键词 水淬渣 贫化 浮选 Copper Water quenched slag Impoverishment Flotation
  • 相关文献

参考文献9

二级参考文献20

共引文献85

同被引文献161

引证文献11

二级引证文献111

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部