摘要
研究了压水堆主回路铁的模拟腐蚀产物在柠檬酸、过氧化氢、柠檬酸过氧化氢的水溶液中的溶解特性,结果表明:铁模拟腐蚀产物在柠檬酸水液中的溶解量随柠檬酸浓度增加而增大,随温度的升高而增大,在60℃不同pH值时溶解量值的排列次序为pH3.50>pH4.00>pH3.00>pH4.50>pH2.33;铁模拟腐蚀产物在H2O2水溶液中的溶解量远小于柠檬酸水溶液中的相应值,60℃时溶解量明显小于70℃、80℃时的溶解量;共存的H2O2降低柠檬酸水溶液对铁模拟腐蚀产物的溶解量.
The studies on the dissolution characteristics of simulated corrosion product of iron on pressurized water reactor primary coolant loops in aqueous solution of citric acid,hydrogen peroxide and citric acid-hydrogen peroxide have been performed.The results show that the protion of the dissolved simulated corrosion product in citric acid aqueous solution increases with a rise in citric acid concentration and temperature.The portions of the pro ducts that dissolve at different pH values in 60 ℃ can be sized as pH 3.50>pH4.00>pH 3.00>pH4.50>pH2.33.it is shown that the portion of the dissolved simulated corrosion products in hydrogen peroxide aqueous solution is smaller that the corresponding value in citric acid aqueous solution,the portion in 60 ℃ is less than in 70 ℃ and 80 ℃,and that coexisting hydrogen peroxide reduces quantity of dissolved simulated corrosion products in citric acid aqueous solution.
出处
《湘潭大学自然科学学报》
CAS
CSCD
1998年第1期62-66,共5页
Natural Science Journal of Xiangtan University
基金
核工业部科学基金
关键词
压水堆
主冷却剂回路
在役去污
溶解性
铁
腐蚀
pressurized water reactor
primary coolant loop,inservice decontamination,citric vacid,hydrogen peroxide,dissolubility