摘要
系统阐述了渣油焦化过程中细纤维组织形成的规律,并分析了影响细纤维组织形成的因素,指出适合的转化温度,升温速度和较高的压力,有利于生成质量较好的针状焦,为生产优质针状石油焦指明了方向。
The formation of fibrous tissue during residue delayed coking was described, and the affecting factors of fine fibrous tissues formation was analyzed. The right transformation temperature, warm up speed and higher pressure were good to generate better needle coke, and the direction for production of high-quality needle-like petroleum coke was pointed out.
出处
《广州化工》
CAS
2008年第4期44-45,共2页
GuangZhou Chemical Industry