在40t钢包炉内喂Al线和Ca-Si线,结果表明,Al的平均回收率为66.10%,Ca-Si的平均回收率为57.38%。
The technology of feeding aluminium and calcium-silicon wires into a 40t ladle furnace was developed. The practice showed that the average recovery rate of aluminium reached 66.01% and the recovery rate of calcium-silicon 57.38% which aided to improve the quality of continuous cast slabs.