期刊文献+

某高砷金矿氰化试验研究 被引量:7

Experimental Study on the Cyanidation of Gold Ore containing High Content of Arsenic
下载PDF
导出
摘要 某高砷金矿中金的品位为17g/t-18g/t,砷的质量分数为20.1%-20.5%范围,硫的质量分数为18.46%,铅的质量分数为3.05%。金主要被砷化物及硫化物包裹不易氰化浸出。金矿直接焙烧后,金的氰化浸出率为56.17%,加入助剂焙烧后,金的氰化浸出率为81.48%以内。若在氰化反应体系中加入2?/t增浸剂后,金的氰化浸出率为87%-90%,金的氰化浸出速度得到提高。 The content of gold of certain gold ore containing high content of arsenic is 17g/t - 18g/ t, and the gold ore contains 20.1% -20.5% (mass fraction) arsenic, 18.46% sulfur and 3.05% lead, and gold is hardly cyanide leached mainly since parceled up by arsenide and sulphuret. The gold cyanide leaching rate is 56.17 % by direct roasting, but within 81.48 % with addition of auxiliary agent, then reaches as high as 87% -90% with addition of 2kg/t leaching agent and improves the velocity of cyanidation as well.
出处 《黄金科学技术》 2007年第2期43-46,共4页 Gold Science and Technology
关键词 金矿 焙烧 助剂 增浸剂 gold ore masting auxiliary agent leaching agent
  • 相关文献

参考文献1

二级参考文献4

共引文献2

同被引文献38

引证文献7

二级引证文献27

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部