摘要
介绍了消除φ140mm自动轧管机组轧制薄壁管的纵向壁厚不均的经验。试验证明,在自动轧管机轧制之前采用毛管温度补偿方法可使纵向壁厚不均从0.3下降到0.06mm。
The experiences with eliminating non-uniform longitudinal wall thickness in thin-walled tube rolling on a φ140mm plug mill are described and the experiment shows that the adoption of shell temperature compensation before rolling makes it possible to improve non-uniform longitudinal wall thickness from 0.3mm down to 0.06mm.
出处
《钢管》
CAS
1990年第6期58-59,共2页
Steel Pipe