摘要
通过对木段旋切时的受力状况进行分析及计算,指出单板厚度不均,即中间薄,两边厚,是旋切时木段产生弯曲挠度所致。通过实验也证实了这个结论。并指出旋切时采用防弯压辊是提高单板旋切精度,进而提高胶合板厚高均匀性的关键。建议采用带有防弯装置的旋切机生产单板。
Through analysis and calculation of suffer force condition in peeling log, this article pointed out the peeling thickness uneven, that is the outer sides are thick but the middle is thin, is result of the bending deflection in peeling log. The result has been confirmed by experiment. Adopting the anti-bend press roll is the key to improve the precision of veneer peeling and the thickess eveneess of the plywood. Rotary cut machine with anti-bend press roll should be adopted in veneer producing for saving wood resources.
出处
《东北林业大学学报》
CAS
CSCD
北大核心
1997年第2期75-77,共3页
Journal of Northeast Forestry University
关键词
木板
单板旋切
受力
防弯压辊
Veneer peeling
Force analysis
Anti-bend press roll