摘要
系统阐述了加气混凝土砌块墙体裂缝的基本特征,包括裂缝的6种形式以及裂缝分类,从材料自身、砌筑与抹面砂浆、结构、施工以及工期和环境等方面分析了墙体裂缝成因,并提出了相关防治措施和建议。
The basic characteristic of aerated concrete wall crack has been expounded systematically including six crack types and classification of crack, the reason of wall crack is analyzed from following aspects: material, masonry and piaster mortar, configuration, construction, time limit and environment for a project, and give some measures and advise for prevent crack.
出处
《新型建筑材料》
北大核心
2007年第3期5-9,共5页
New Building Materials
基金
重庆市科学技术项目(城科字2005第18号)
关键词
加气混凝土砌块
墙体裂缝
成因分析
防治措施
aerated concrete block
wall crack
genetic analysis
prevention measures