摘要 研究了定向有机玻璃在不同温度下的拉伸断裂行为,探讨了定向有机玻璃拉伸行为与温度的关系。结果表明:随温度升高,定向有机玻璃的拉伸强度和拉伸模量降低,断裂伸长率增加,材料由刚而脆变得软而韧。不同温度下定向有机玻璃的断裂特征差别显著,在23℃时分层断裂特征最明显,在-55℃时主要为礼花状放射特征,而在80℃时主要为韧性断裂特征。 Tensile fracture behavior of directional PMMA at different temperature is investigated. And the relationship between tensile behavior and temperature is discussed. The result shows with the temperature increasing, tensile strength and modulus decreases but elongation increase and material properties change from rigidity to flexibility. Fracture characteristics of directional PMMA are obviously different at different temperature. Frauture faces exhibit delamination features at 23℃ ,fireworks fractures at -55℃ and flexibility features at 80℃.
出处 《航空材料学报》 EI CAS CSCD 2006年第5期106-108,共3页 Journal of Aeronautical Materials
关键词 定向有机玻璃 断裂 温度 结构 Directional PMMA fracture temperature structure
  • 相关文献

参考文献4

二级参考文献9

  • 1李强,贺子如,宋名实,唐敖庆.玻璃态高聚物细观损伤断裂统计力学[J].力学进展,1995,25(4):451-470. 被引量:17
  • 2张志林.教8飞机活动舱盖玻璃破裂原因分析总结[M].南昌:江西洪都航空工业集团有限责任公司650所,1998.. 被引量:1
  • 3许凤和.有机玻璃疲劳和断口图谱[M].北京:科学出版社,1987.58-78. 被引量:1
  • 4李强,中国科学.A,1995年,20卷,10期,1082页 被引量:1
  • 5Xing X S,Eng Fract Mech,1990年,37卷,1099页 被引量:1
  • 6Zhang Z D,J Appl Phys,1983年,54卷,5568页 被引量:1
  • 7张志林,教8飞机活动舱盖玻璃破裂原因分析总结,1998年 被引量:1
  • 8许凤和,有机玻璃疲劳和断口图谱,1987年,58页 被引量:1
  • 9许凤和等.航空非金属件失效分析[M]科学出版社,1993. 被引量:1

共引文献8

同被引文献161

引证文献22

二级引证文献72

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部