摘要
用中温水热法合成了类水滑石[Cd_xMg_(6-x)Al_2(OH)_(16)]^(2+)[S·2H_2O]^(2-),探讨了pH值、投入Cd^(2+)离子的量以及硫化时间等条件对合成的影响,并用XRD、FT-IR、DTA-TG等手段进行了表征,找出了合成层间嵌入S^(2-)离子的含Cd类水滑石的最佳条件.
Hydrotalcite-like [Cd_xMg_(6-x)Al_2(OH)_16] ̄2+[S·2H_2O] ̄2-was synthesized hydrothermally and characterized by means of XRD,FT-IR,DTA-TG etc.,The influence of pH,Cd ̄2+ ionic concentration and sulphuration time on the synthesis was studied.The synthetic optimal conditions are pH=9~10,[Cd ̄2+]/[Mg2+]=1:5~1:9 and sulphuration time 5 min. It is suggested that Mg ̄2+ ions can be only partially substituted by Cd ̄2+ ions in the hydrotalcite-like.