摘要
针对攀钢线材厂现有粗中轧工艺存在的轧件冲塞导卫,倒料,摆料,主机跳闸,断辊等主要问题,不断拟定改进措施进行实施,通过关键架次增设短应力轧机、增设滚动导卫,增设粗轧飞剪,不断优化孔型、导卫参数,取得了显著效果,实践证明是可行的。
In view of the existing problem of the current roughing middle mill technology in PZH Iron and steel group.co.wire rod factory,establishing the series improvement measure.Passing to added sortie short of the rolling mill in response.Added the rolling guide.Added shearing of the roughing mill,continuously excellent turn the passing and parameter of the guide.after adopting these measures,homework rate of the rolling mill is further to increase.
出处
《四川冶金》
CAS
2005年第2期10-13,共4页
Sichuan Metallurgy