摘要  为了对比纳米HA与大颗粒或大晶粒HA作为骨填充材料在动物体内的实验效果,通过改变烧结工艺来获得大颗粒或大晶粒HA.扫描电镜检测结果表明,烧结温度对粒子尺寸的影响最为敏感:低于800℃烧结时,粒子长大缓慢甚至没有长大现象;超过900℃后,粒子迅速长大;1200℃烧结时,随烧结时间延长,晶粒呈现不规则长大,并出现二次再结晶现象. In order to compare the difference between nano-HAp and bigger size of HAp as the bone-implanting materials in the animals, the sintering process was adjusted and the bigger size of HAp was gotten. The influence of sintering temperature and time on the size was investigated:the size of particle is the most sensitive to the sintering temperature, in low sintering temperature extent where the particles grow slowly or even stop, while the particle could be more quickly and would show recrystallization when it exceeds some certain temperature. It also appears the phenomenon of the recrystallization with the increase of sintering time.
出处 《佳木斯大学学报(自然科学版)》 CAS 2005年第1期85-87,共3页 Journal of Jiamusi University:Natural Science Edition
关键词 HA 烧结温度 烧结时间 the synthesis of wet-way HA sintering temperature sintering time
  • 引文网络
  • 相关文献

参考文献6

二级参考文献29

  • 1(日)大矢晴彦 张谨(译).分离的科学与技术[M].北京:中国轻工业出版社,1999,8.. 被引量:1
  • 2陆水玉 金红芳.表面及界面分析的一种有效手段科学(上海)[M].,1995,47(3).57. 被引量:1
  • 3韩颖超 王新宇 李世普.Guisuan Yan Xuebao(J Chin Ceram Soc ),2002,30(3):357-357. 被引量:1
  • 4廖其龙 徐光亮 伊光福.Gongneng Cailiao ( Functional Materials),2002,33(3):338-338. 被引量:1
  • 5徐光亮 聂轶霞光 赖振宇.Wuji Cailiao Xuebao ( J Inorg Mater ),2002,17(3):600-600. 被引量:1
  • 6Narasaraju T S B, Lahire P. Curr Sci, 1998, 51,772. 被引量:1
  • 7Cheng H M, Ma J M, Zhao Z G. Chem Mater, 1995, 7(4), 663. 被引量:1
  • 8Montenero A, Gnappi G, Ferrari F. J Mater Sci, 2000,35, 2791. 被引量:1
  • 9George C K, Alexandros P K, Athanasios K. J Colloid Int Sci, 2003, 259, 254. 被引量:1
  • 10Elliot I C, Young R A. Nature, 1967, 214, 904. 被引量:1

共引文献41

同被引文献26

引证文献4

二级引证文献10

;
使用帮助 返回顶部