Investigating the stress corrosion cracking of a biodegradable Zn-0.8 wt%Li alloy in simulated body fluid 被引量:5
1
作者 Guan-Nan Li Su-Ming Zhu +2 位作者 Jian-Feng Nie Yufeng Zheng Zhili Sun 《Bioactive Materials》 SCIE 2021年第5期1468-1478,共11页
Stress corrosion cracking(SCC)may lead to brittle,unexpected failure of medical devices.However,available researches are limited to Mg-based biodegradable metals(BM)and pure Zn.The stress corrosion behaviors of newly-... Stress corrosion cracking(SCC)may lead to brittle,unexpected failure of medical devices.However,available researches are limited to Mg-based biodegradable metals(BM)and pure Zn.The stress corrosion behaviors of newly-developed Zn alloys remain unclear.In the present work,we conducted slow strain rate testing(SSRT)and constant-load immersion test on a promising Zn-0.8 wt%Li alloy in order to investigate its SCC susceptibility and examine its feasibility as BM with pure Zn as control group.We observed that Zn-0.8 wt%Li alloy exhibited low SCC susceptibility.This was attributed to variations in microstructure and deformation mechanism after alloying with Li.In addition,both pure Zn and Zn-0.8 wt%Li alloy did not fracture over a period of 28 days during constant-load immersion test.The magnitude of applied stress was close to physiological condition and thus,we proved the feasibility of both materials as BM. 展开更多
关键词 Biodegradable metals Zn-0.8 wt%li alloy Stress corrosion Slow strain rate testing Constant-load immersion test
原文传递
NiAl基多相金属间化合物在LiCl-Li_2O熔盐中的腐蚀行为
2
作者 刘瑞岩 孙岩 +3 位作者 张俊善 郭建亭 祝美丽 王秀敏 《材料科学与工程学报》 CAS CSCD 北大核心 2003年第6期845-850,共6页
利用浸没法腐蚀实验研究了NiAl 2 8Cr 5 8Mo 0 2Hf和Ni 2 5Al 15Cr合金在 75 0℃下 ,LiCl 10wt%Li2 O熔盐中的腐蚀行为。实验结果表明 :NiAl 2 8Cr 5 8Mo 0 2Hf和Ni 2 5Al 15Cr两种合金在 75 0℃ ,LiCl 10wt%Li2 O熔盐中的腐蚀产物... 利用浸没法腐蚀实验研究了NiAl 2 8Cr 5 8Mo 0 2Hf和Ni 2 5Al 15Cr合金在 75 0℃下 ,LiCl 10wt%Li2 O熔盐中的腐蚀行为。实验结果表明 :NiAl 2 8Cr 5 8Mo 0 2Hf和Ni 2 5Al 15Cr两种合金在 75 0℃ ,LiCl 10wt%Li2 O熔盐中的腐蚀产物都为LiCrO2 、LiAlO2 ,NiAl 2 8Cr 5 8Mo 0 2Hf合金的耐蚀性能优于Ni 2 5Al 15Cr合金 ,主要是由于NiAl 2 8Cr 5 8Mo 0 2Hf合金两相里的NiAl(β)相的腐蚀滞后于Cr(Mo)相的腐蚀。在此种熔盐腐蚀环境下 ,两种合金形成的腐蚀层都是非保持性的 。 展开更多
关键词 liCl-li2O熔盐 NIAL合金 核燃料 环境保护 核能工业 耐腐蚀性能