我国煤矿锚杆强度偏低,对冲击吸收功没有指标要求。通过对煤矿井下锚杆破断情况调查及分析,发现锚杆破断强度低、夹杂物含量高、冲击韧性不足、抗冲击能力不够是造成杆体脆断的重要原因,冲击韧性值低是发生脆断的材质内在因素。介绍了...我国煤矿锚杆强度偏低,对冲击吸收功没有指标要求。通过对煤矿井下锚杆破断情况调查及分析,发现锚杆破断强度低、夹杂物含量高、冲击韧性不足、抗冲击能力不够是造成杆体脆断的重要原因,冲击韧性值低是发生脆断的材质内在因素。介绍了超高强热处理锚杆的主要工艺,对超高强热处理锚杆材料进行了拉伸、拉扭弯及力学性能实验室试验,数据显示这种材料在受拉、扭、弯的情况下可以承受较高的载荷,特别是冲击吸收功指标,是热轧强力锚杆的数倍。在潞安集团漳村煤矿动压巷道进行了井下现场试验,对超高强热处理锚杆受力情况进行了监测,锚杆施加预紧扭矩后初始预紧力为52~98 k N,受力稳定后最大受力为223 k N,小于其破断极限,矿压监测数据表明,支护系统有效地控制了围岩的变形,支护效果良好。展开更多
The surface properties of oxidic supports and their interaction with the supported metals play critical roles in governing the catalytic activities of oxide‐supported metal catalysts.When metals are supported on redu...The surface properties of oxidic supports and their interaction with the supported metals play critical roles in governing the catalytic activities of oxide‐supported metal catalysts.When metals are supported on reducible oxides,dynamic surface reconstruction phenomena,including strong metal–support interaction(SMSI)and oxygen vacancy formation,complicate the determination of the structural–functional relationship at the active sites.Here,we performed a systematic investigation of the dynamic behavior of Au nanocatalysts supported on flame‐synthesized TiO_(2),which takes predominantly a rutile phase,using CO oxidation above room temperature as a probe reaction.Our analysis conclusively elucidated a negative correlation between the catalytic activity of Au/TiO_(2) and the oxygen vacancy at the Au/TiO_(2) interface.Although the reversible formation and retracting of SMSI overlayers have been ubiquitously observed on Au/TiO_(2) samples,the catalytic consequence of SMSI remains inconclusive.Density functional theory suggests that the electron transfer from TiO_(2) to Au is correlated to the presence of the interfacial oxygen vacancies,retarding the catalytic activation of CO oxidation.展开更多
Ordered mesoporous Mn2O3 (meso‐Mn2O3) and meso‐Mn2O3‐supported Pd, Pt, and Pd‐Pt alloy x(PdyPt)/meso‐Mn2O3; x = (0.10?1.50) wt%; Pd/Pt molar ratio (y) = 4.9?5.1 nanocatalysts were prepared using KIT‐6‐templated...Ordered mesoporous Mn2O3 (meso‐Mn2O3) and meso‐Mn2O3‐supported Pd, Pt, and Pd‐Pt alloy x(PdyPt)/meso‐Mn2O3; x = (0.10?1.50) wt%; Pd/Pt molar ratio (y) = 4.9?5.1 nanocatalysts were prepared using KIT‐6‐templated and poly(vinyl alcohol)‐protected reduction methods, respectively.The meso‐Mn2O3 had a high surface area, i.e., 106 m2/g, and a cubic crystal structure. Noble‐metalnanoparticles (NPs) of size 2.1?2.8 nm were uniformly dispersed on the meso‐Mn2O3 surfaces. AlloyingPd with Pt enhanced the catalytic activity in methane combustion; 1.41(Pd5.1Pt)/meso‐Mn2O3gave the best performance; T10%, T50%, and T90% (the temperatures required for achieving methaneconversions of 10%, 50%, and 90%) were 265, 345, and 425 °C, respectively, at a space velocity of20000 mL/(g?h). The effects of SO2, CO2, H2O, and NO on methane combustion over1.41(Pd5.1Pt)/meso‐Mn2O3 were also examined. We conclude that the good catalytic performance of1.41(Pd5.1Pt)/meso‐Mn2O3 is associated with its high‐quality porous structure, high adsorbed oxygen species concentration, good low‐temperature reducibility, and strong interactions between Pd‐Pt alloy NPs and the meso‐Mn2O3 support.展开更多
Ruthenium(Ru)has been regarded as one of the most promising alternatives to substitute Pt for catalyzing alkaline hydrogen evolution reaction(HER),owing to its inherent high activity and being the cheapest platinum-gr...Ruthenium(Ru)has been regarded as one of the most promising alternatives to substitute Pt for catalyzing alkaline hydrogen evolution reaction(HER),owing to its inherent high activity and being the cheapest platinum-group metal.Herein,based on the idea of strong metal–support interaction(SMSI)regulation,Ru/TiN catalysts with different degrees of TiN overlayer over Ru nanoparticles were fabricated,which were applied to the alkaline electrolytic water.Characterizations reveal that the TiN overlayer would gradually encapsulate the Ru nanoparticles and induce more electron transfer from Ru nanoparticles to TiN support by the Ru–N–Ti bond as the SMSI degree increased.Further study shows that the exposed Ru–TiN interfaces greatly promote the H_(2) desorption capacity.Thus,the Ru/TiN-300 with a moderate SMSI degree exhibits excellent HER performance,with an overpotential of 38 mV at 10 mA cm^(−2).Also,due to the encapsulation role of TiN overlayer on Ru nanoparticles,it displays super long-term stability with a very slight potential change after 24 h.This study provides a deep insight into the influence of the SMSI effect between Ru and TiN on HER and offers a novel approach for preparing efficient and stable HER electrocatalysts through SMSI engineering.展开更多
Water electrolysis poses a significant challenge for balancing catalytic activity and stability of oxygen evolution reaction(OER)electrocatalysts.In this study,we address this challenge by constructing asymmetric redo...Water electrolysis poses a significant challenge for balancing catalytic activity and stability of oxygen evolution reaction(OER)electrocatalysts.In this study,we address this challenge by constructing asymmetric redox chemistry through elaborate surface OO–Ru–OH and bulk Ru–O–Ni/Fe coordination moieties within single-atom Ru-decorated defective NiFe LDH nanosheets(Ru@d-NiFe LDH)in conjunction with strong metal-support interactions(SMSI).Rigorous spectroscopic characterization and theoretical calculations indicate that single-atom Ru can delocalize the O 2p electrons on the surface and optimize d-electron configurations of metal atoms in bulk through SMSI.The^(18)O isotope labeling experiment based on operando differential electrochemical mass spectrometry(DEMS),chemical probe experiments,and theoretical calculations confirm the encouraged surface lattice oxygen,stabilized bulk lattice oxygen,and enhanced adsorption of oxygen-containing intermediates for bulk metals in Ru@d-NiFe LDH,leading to asymmetric redox chemistry for OER.The Ru@d-NiFe LDH electrocatalyst exhibits exceptional performance with an overpotential of 230 mV to achieve 10 mA cm^(−2)and maintains high robustness under industrial current density.This approach for achieving asymmetric redox chemistry through SMSI presents a new avenue for developing high-performance electrocatalysts and instills confidence in its industrial applicability.展开更多
Tuning Strong Metal-support Interactions(SMSI)is a key strategy to obtain highly active catalysts,but conventional methods usually enable TiO_(x) encapsulation of noble metal components to minimize the exposure of nob...Tuning Strong Metal-support Interactions(SMSI)is a key strategy to obtain highly active catalysts,but conventional methods usually enable TiO_(x) encapsulation of noble metal components to minimize the exposure of noble metals.This study demonstrates a catalyst preparation method to modulate a weak encapsulation of Pt metal nanoparticles(NPs)with the supported TiO_(2),achieving the moderate suppression of SMSI effects.The introduction of silica inhibits this encapsulation,as reflected in the characterization results such as XPS and HRTEM,while the Ti^(4+) to Ti^(3+) conversion due to SMSI can still be found on the support surface.Furthermore,the hydrogenation of cinnamaldehyde(CAL)as a probe reaction revealed that once this encapsulation behavior was suppressed,the adsorption capacity of the catalyst for small molecules like H_(2) and CO was enhanced,which thereby improved the catalytic activity and facilitated the hydrogenation of CAL.Meanwhile,the introduction of SiO_(2) also changed the surface structure of the catalyst,which inhibited the occurrence of the acetal reaction and improved the conversion efficiency of C=O and C=C hydrogenation.Systematic manipulation of SMSI formation and its consequence on the performance in catalytic hydrogenation reactions are discussed.展开更多
The phenomenon of strong metal-support interaction(SMSI)observed in supported metal catalysts,usually accompanied by the formation of the encapsulation layer on metal nanoparticles,has attracted extensive research att...The phenomenon of strong metal-support interaction(SMSI)observed in supported metal catalysts,usually accompanied by the formation of the encapsulation layer on metal nanoparticles,has attracted extensive research attention due to its significance in heterogeneous catalysis.Notably,great progress has been made in recent years in investigating SMSI by in situ transmission electron microscopy(TEM),along with an enhanced comprehension of the underlying mechanisms governing SMSI formation.This emerging topic summarizes recent progress utilizing in situ TEM to study the interaction between metal and support and the relationship between the structure and performance of the supported catalyst under reaction conditions.A brief perspective about the use of in situ TEM for further study of SMSI is also presented,showing prospects in this field that will stimulate further upsurging research in promoting the catalytic efficiency of supported catalysts.展开更多
文摘我国煤矿锚杆强度偏低,对冲击吸收功没有指标要求。通过对煤矿井下锚杆破断情况调查及分析,发现锚杆破断强度低、夹杂物含量高、冲击韧性不足、抗冲击能力不够是造成杆体脆断的重要原因,冲击韧性值低是发生脆断的材质内在因素。介绍了超高强热处理锚杆的主要工艺,对超高强热处理锚杆材料进行了拉伸、拉扭弯及力学性能实验室试验,数据显示这种材料在受拉、扭、弯的情况下可以承受较高的载荷,特别是冲击吸收功指标,是热轧强力锚杆的数倍。在潞安集团漳村煤矿动压巷道进行了井下现场试验,对超高强热处理锚杆受力情况进行了监测,锚杆施加预紧扭矩后初始预紧力为52~98 k N,受力稳定后最大受力为223 k N,小于其破断极限,矿压监测数据表明,支护系统有效地控制了围岩的变形,支护效果良好。
基金Science and Technology Innovation Program of Hunan Province,Grant/Award Numbers:2020GK2070,2021RC4006Innovation‐Driven Project of Central South University,Grant/Award Number:2020CX008+3 种基金China Scholarship Council(CSC)National Key R&D Program of China,Grant/Award Number:2022YFE0105900National Natural Science Foundation of China,Grant/Award Number:52276093National Research Foundation Singapore,Grant/Award Number:CREATE。
文摘The surface properties of oxidic supports and their interaction with the supported metals play critical roles in governing the catalytic activities of oxide‐supported metal catalysts.When metals are supported on reducible oxides,dynamic surface reconstruction phenomena,including strong metal–support interaction(SMSI)and oxygen vacancy formation,complicate the determination of the structural–functional relationship at the active sites.Here,we performed a systematic investigation of the dynamic behavior of Au nanocatalysts supported on flame‐synthesized TiO_(2),which takes predominantly a rutile phase,using CO oxidation above room temperature as a probe reaction.Our analysis conclusively elucidated a negative correlation between the catalytic activity of Au/TiO_(2) and the oxygen vacancy at the Au/TiO_(2) interface.Although the reversible formation and retracting of SMSI overlayers have been ubiquitously observed on Au/TiO_(2) samples,the catalytic consequence of SMSI remains inconclusive.Density functional theory suggests that the electron transfer from TiO_(2) to Au is correlated to the presence of the interfacial oxygen vacancies,retarding the catalytic activation of CO oxidation.
基金supported by the Ph.D.Program Foundation of Ministry of Education of China(20131103110002)the NNSF of China(21377008)+2 种基金National High Technology Research and Development Program(863 Program,2015AA034603)Foundation on the Creative Research Team Con-struction Promotion Project of Beijing Municipal InstitutionsScientific Research Base Construction-Science and Technology Creation Plat-form-National Materials Research Base Construction~~
文摘Ordered mesoporous Mn2O3 (meso‐Mn2O3) and meso‐Mn2O3‐supported Pd, Pt, and Pd‐Pt alloy x(PdyPt)/meso‐Mn2O3; x = (0.10?1.50) wt%; Pd/Pt molar ratio (y) = 4.9?5.1 nanocatalysts were prepared using KIT‐6‐templated and poly(vinyl alcohol)‐protected reduction methods, respectively.The meso‐Mn2O3 had a high surface area, i.e., 106 m2/g, and a cubic crystal structure. Noble‐metalnanoparticles (NPs) of size 2.1?2.8 nm were uniformly dispersed on the meso‐Mn2O3 surfaces. AlloyingPd with Pt enhanced the catalytic activity in methane combustion; 1.41(Pd5.1Pt)/meso‐Mn2O3gave the best performance; T10%, T50%, and T90% (the temperatures required for achieving methaneconversions of 10%, 50%, and 90%) were 265, 345, and 425 °C, respectively, at a space velocity of20000 mL/(g?h). The effects of SO2, CO2, H2O, and NO on methane combustion over1.41(Pd5.1Pt)/meso‐Mn2O3 were also examined. We conclude that the good catalytic performance of1.41(Pd5.1Pt)/meso‐Mn2O3 is associated with its high‐quality porous structure, high adsorbed oxygen species concentration, good low‐temperature reducibility, and strong interactions between Pd‐Pt alloy NPs and the meso‐Mn2O3 support.
基金supported by the National Natural Science Foundation of China(Grant Nos.22075159,22002066)Shandong Taishan Scholars Project(Grant Nos.ts20190932,tsqn202103058)+1 种基金Open Fund of Hubei Key Laboratory of Processing and Application of Catalytic Materials(Grant No.202203404)Postdoctoral Applied Research Project in Qingdao,and the Youth Innovation Team Project of Shandong Provincial Education Department(Grant No.2019KJC023).
文摘Ruthenium(Ru)has been regarded as one of the most promising alternatives to substitute Pt for catalyzing alkaline hydrogen evolution reaction(HER),owing to its inherent high activity and being the cheapest platinum-group metal.Herein,based on the idea of strong metal–support interaction(SMSI)regulation,Ru/TiN catalysts with different degrees of TiN overlayer over Ru nanoparticles were fabricated,which were applied to the alkaline electrolytic water.Characterizations reveal that the TiN overlayer would gradually encapsulate the Ru nanoparticles and induce more electron transfer from Ru nanoparticles to TiN support by the Ru–N–Ti bond as the SMSI degree increased.Further study shows that the exposed Ru–TiN interfaces greatly promote the H_(2) desorption capacity.Thus,the Ru/TiN-300 with a moderate SMSI degree exhibits excellent HER performance,with an overpotential of 38 mV at 10 mA cm^(−2).Also,due to the encapsulation role of TiN overlayer on Ru nanoparticles,it displays super long-term stability with a very slight potential change after 24 h.This study provides a deep insight into the influence of the SMSI effect between Ru and TiN on HER and offers a novel approach for preparing efficient and stable HER electrocatalysts through SMSI engineering.
基金supported by the Guangdong Basic and Applied Basic Research Foundation(2021B1515120072)the Natural Science Foundation of China(22279096 and T2241003)the Fundamental Research Funds for the Central Universities(WUT:2023IVA094).
文摘Water electrolysis poses a significant challenge for balancing catalytic activity and stability of oxygen evolution reaction(OER)electrocatalysts.In this study,we address this challenge by constructing asymmetric redox chemistry through elaborate surface OO–Ru–OH and bulk Ru–O–Ni/Fe coordination moieties within single-atom Ru-decorated defective NiFe LDH nanosheets(Ru@d-NiFe LDH)in conjunction with strong metal-support interactions(SMSI).Rigorous spectroscopic characterization and theoretical calculations indicate that single-atom Ru can delocalize the O 2p electrons on the surface and optimize d-electron configurations of metal atoms in bulk through SMSI.The^(18)O isotope labeling experiment based on operando differential electrochemical mass spectrometry(DEMS),chemical probe experiments,and theoretical calculations confirm the encouraged surface lattice oxygen,stabilized bulk lattice oxygen,and enhanced adsorption of oxygen-containing intermediates for bulk metals in Ru@d-NiFe LDH,leading to asymmetric redox chemistry for OER.The Ru@d-NiFe LDH electrocatalyst exhibits exceptional performance with an overpotential of 230 mV to achieve 10 mA cm^(−2)and maintains high robustness under industrial current density.This approach for achieving asymmetric redox chemistry through SMSI presents a new avenue for developing high-performance electrocatalysts and instills confidence in its industrial applicability.
基金the National Natural Science Foundation of China(21576291,22003076)National Natural Science Foundation of China-Outstanding Youth foundation(22322814)the Fundamental Research Funds for the Central Universities(23CX03007A,22CX06012A)are gratefully acknowledge。
文摘Tuning Strong Metal-support Interactions(SMSI)is a key strategy to obtain highly active catalysts,but conventional methods usually enable TiO_(x) encapsulation of noble metal components to minimize the exposure of noble metals.This study demonstrates a catalyst preparation method to modulate a weak encapsulation of Pt metal nanoparticles(NPs)with the supported TiO_(2),achieving the moderate suppression of SMSI effects.The introduction of silica inhibits this encapsulation,as reflected in the characterization results such as XPS and HRTEM,while the Ti^(4+) to Ti^(3+) conversion due to SMSI can still be found on the support surface.Furthermore,the hydrogenation of cinnamaldehyde(CAL)as a probe reaction revealed that once this encapsulation behavior was suppressed,the adsorption capacity of the catalyst for small molecules like H_(2) and CO was enhanced,which thereby improved the catalytic activity and facilitated the hydrogenation of CAL.Meanwhile,the introduction of SiO_(2) also changed the surface structure of the catalyst,which inhibited the occurrence of the acetal reaction and improved the conversion efficiency of C=O and C=C hydrogenation.Systematic manipulation of SMSI formation and its consequence on the performance in catalytic hydrogenation reactions are discussed.
基金the support from the National Natural Science Foundation of China(22376062)the Science and Technology Commission of Shanghai Municipality(22ZR1415700)+1 种基金Shanghai Rising-star Program(20QA1402400)and the Fundamental Research Funds for the Central Universities,Additional support was provided by the Frontiers Science Center for Materiobiology and Dynamic Chemistry and the Feringa Nobel Prize Scientist Joint Research Center at East China University of Science and Technology。
文摘The phenomenon of strong metal-support interaction(SMSI)observed in supported metal catalysts,usually accompanied by the formation of the encapsulation layer on metal nanoparticles,has attracted extensive research attention due to its significance in heterogeneous catalysis.Notably,great progress has been made in recent years in investigating SMSI by in situ transmission electron microscopy(TEM),along with an enhanced comprehension of the underlying mechanisms governing SMSI formation.This emerging topic summarizes recent progress utilizing in situ TEM to study the interaction between metal and support and the relationship between the structure and performance of the supported catalyst under reaction conditions.A brief perspective about the use of in situ TEM for further study of SMSI is also presented,showing prospects in this field that will stimulate further upsurging research in promoting the catalytic efficiency of supported catalysts.