期刊文献+
共找到2篇文章
< 1 >
每页显示 20 50 100
Recovery of vanadium and molybdenum from spent petrochemical catalyst by microwave-assisted leaching 被引量:11
1
作者 Zhi-yuan Ma Yong Liu +2 位作者 Ji-kui Zhou Mu-dan Liu Zhen-zhen Liu 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2019年第1期33-40,共8页
The study of the leaching of vanadium(V) and molybdenum(Mo) from spent petrochemical catalysts in sodium hydroxide(NaO H) medium was performed using two approaches, namely, conventional leaching and microwave-assisted... The study of the leaching of vanadium(V) and molybdenum(Mo) from spent petrochemical catalysts in sodium hydroxide(NaO H) medium was performed using two approaches, namely, conventional leaching and microwave-assisted leaching methods. The influence of microwave power, leaching time, leaching temperature, and NaOH concentration on the leaching efficiency of spent petrochemical catalyst was investigated. Under microwave-assisted conditions(600 W, 10 min, 90°C, 2.0 mol·L^(-1) NaOH, and 0.20 g·mL^(-1) solid–liquid ratio), the leaching efficiencies of V and Mo reached 94.35% and 96.23%, respectively. It has been confirmed that microwave energy has considerable potential to enhance the efficiency of the leaching process and reduce the leaching time. It is suggested that the enhancement of the leaching efficiencies of V and Mo can be attributed to the existence of a thermal gradient between solid and liquid and the generation of cracks on the mineral surface. 展开更多
关键词 microwave spent petrochemical catalyst VANADIUM MOLYBDENUM
下载PDF
废石化催化剂碱浸液中钒的分离提取研究 被引量:1
2
作者 马致远 刘勇 +2 位作者 吕建芳 吕先谨 周吉奎 《矿冶工程》 CAS CSCD 北大核心 2022年第6期133-138,共6页
以废石化催化剂碱性浸出液为研究对象,进行了N263三级逆流萃取+超声波一级NH4Cl反萃+三级NaOH、NaCl逆流反萃工艺研究。结果表明,优化萃取条件为:初始pH值8.5、萃取体系30%N263+5%仲辛醇+65%磺化煤油、萃取时间3 min、相比O/A=1∶1;一... 以废石化催化剂碱性浸出液为研究对象,进行了N263三级逆流萃取+超声波一级NH4Cl反萃+三级NaOH、NaCl逆流反萃工艺研究。结果表明,优化萃取条件为:初始pH值8.5、萃取体系30%N263+5%仲辛醇+65%磺化煤油、萃取时间3 min、相比O/A=1∶1;一段反萃优化条件为:NH4Cl浓度2.0 mol/L、反萃相比O/A=5∶2、超声波功率500 W、反萃时间2 min;二段反萃优化条件为:NaOH浓度1.0 mol/L、NaCl浓度0.5 mol/L、反萃相比O/A=3∶2、反萃时间3 min。以上优化条件下对浸出液进行钒的提取,钒萃取率和反萃率分别为99.15%和99.36%,对一段和二段反萃液进行钒产品回收,可分别获得高纯V2O5产品(>99.9%)和普通V2O5产品(>99%)。 展开更多
关键词 废石化催化剂 萃取 超声波 反萃
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部