期刊文献+
共找到4篇文章
< 1 >
每页显示 20 50 100
碘三离子后处理对钙钛矿太阳电池的影响研究 被引量:8
1
作者 李星宇 董海悦 +3 位作者 夏天 刘玮婷 姚迪圣 龙飞 《太阳能学报》 EI CAS CSCD 北大核心 2023年第3期409-414,共6页
采用碘三离子(I3-)作为提升钙钛矿太阳电池性能的界面修饰材料,对钙钛矿体相及上层空穴传输材料的接触界面进行修饰和改性,钝化光活性层上表面缺陷,以优化光电转换器件的转换效率。由反溶剂法和后处理的形式,制备平面异质结电池,运用该... 采用碘三离子(I3-)作为提升钙钛矿太阳电池性能的界面修饰材料,对钙钛矿体相及上层空穴传输材料的接触界面进行修饰和改性,钝化光活性层上表面缺陷,以优化光电转换器件的转换效率。由反溶剂法和后处理的形式,制备平面异质结电池,运用该界面钝化策略改善后的器件效率达到18.9%,且电池的稳定性也得到增强,600 h后仅有5%的性能衰减。通过物相和光电性质等表征与测试,系统地研究电池的形貌及性能参数,探究不同浓度的I3-对器件性能的影响作用和机理。研究发现,该缺陷钝化策略对钙钛矿膜层进行处理后,能有效改善钙钛矿材料的结晶性,减少其表面陷阱态缺陷,降低钙钛矿与空穴传输层的载流子界面传输势垒,且I3-与钙钛矿能形成钝化层,起到隔绝水氧的作用,使其稳定性得到改善。 展开更多
关键词 钙钛矿太阳电池 缺陷钝化 反溶剂 界面修饰 碘三离子 后处理 稳定性
下载PDF
Residual solvent extraction via chemical displacement for efficient and stable perovskite solar cells 被引量:3
2
作者 Min Fang Lei Tao +10 位作者 Wen Wu Qi Wei Yingdong Xia Ping Li Xueqin Ran Qi Zhong Guichuan Xing Lin Song Peter Müller-Buschbaum Hui Zhang Yonghua Chen 《Journal of Energy Chemistry》 SCIE EI CAS CSCD 2021年第10期8-14,I0001,共8页
Solvent residue is inevitable to occur in solution processed thin films,but its influence on the thin film quality has not been identified and addressed to date.Methylammonium acetate(MAAc)ionic liquid has recently be... Solvent residue is inevitable to occur in solution processed thin films,but its influence on the thin film quality has not been identified and addressed to date.Methylammonium acetate(MAAc)ionic liquid has recently been realized as an environmentally friendly solvent for solution processed perovskites.The specific high viscosity,low vapor pressure and strong association with perovskite precursor of the MAAc solvent is a double-edged sword,which endowed an advantageously ambient air operational and anti-solvent free perovskite deposition,but the MAAc is likely to be retained within the film and bring in detrimental effects on device performance of the corresponding solar cells.Herein,we reported a novel route to eliminate the residual solvent via a facial hydrochloric acid(HCl)annealing post-treatment(HAAP).In particular,chemical displacement reaction between the incorporated HCl and residual MAAc can be initiated to form volatile MACl and HAc,efficiently extracting MAAc residue.In the meanwhile,the stimulated mass transport via downward penetration and upward escape can trigger secondary perovskite growth with enlarged grain size and smoothened surface,leading to reduced defect state and improved interfacial contact intimacy,and also partial chloride ions are able to enter the crystal lattice to stabilize perovskite phase structure.As a result,a champion efficiency up to20.78%originating from enhanced Voc was achieved,and more than 96%of its initial efficiency can be maintained after 1000 h shelf-storage. 展开更多
关键词 PEROVSKITE Solar cells solvent residue Methylammonium acetate post-treatment Chemical displacement
下载PDF
溶剂处理对PPESK中空纤维膜O_2/N_2分离性能的影响
3
作者 杨大令 朱瑞霞 +1 位作者 张守海 蹇锡高 《现代化工》 CAS CSCD 北大核心 2011年第S1期130-133,共4页
研究了不同溶剂处理对PPESK中空纤维非对称膜O2/N2分离性能的影响。通过PPESK的二次溶胀、溶解过程,弥补或减少膜表面的缺陷孔,降低表面孔隙率,从而提高中空纤维非对称膜的皮层致密性。实验结果表明,通过溶剂处理,O2/N2分离系数由0.94... 研究了不同溶剂处理对PPESK中空纤维非对称膜O2/N2分离性能的影响。通过PPESK的二次溶胀、溶解过程,弥补或减少膜表面的缺陷孔,降低表面孔隙率,从而提高中空纤维非对称膜的皮层致密性。实验结果表明,通过溶剂处理,O2/N2分离系数由0.94提高到1.00以上,并且长时间测试仍然具有稳定的分离性能。 展开更多
关键词 溶剂处理 非对称膜 孔隙率 O2/N2分离系数
下载PDF
溶剂处理提高聚砜非对称中空纤维膜气体分离性能
4
作者 刘丽 陆文军 +1 位作者 王海 马庙江 《膜科学与技术》 CAS CSCD 1996年第2期69-74,共6页
考察了溶剂处理对聚砜非对称中空纤维膜气体分离性能的影响.利用溶剂在膜表面缺陷孔中溶胀聚砜的作用,调整膜表面孔分布,降低表面孔隙率。
关键词 溶剂处理 分离 中空纤维膜 聚砜 膜分离
下载PDF