低温陈化法制备SO_4^(2-)/WO_3-TiO_2固体超强酸及性能研究 被引量:2
1
作者 陈同云 郑明东 胡克良 《无机化学学报》 SCIE CAS CSCD 北大核心 2004年第8期941-945,共5页
The SO42-/WO3-TiO2 solid superacid samples have been prepared by ageing at low temperature. The acidity of samples were determined with flowing indicator method, and the characterization of the samples were performed ... The SO42-/WO3-TiO2 solid superacid samples have been prepared by ageing at low temperature. The acidity of samples were determined with flowing indicator method, and the characterization of the samples were performed by IR, XPS and XRD. The samples were used in the esterification of acetic acid and glycerol. The results show that the sample aged at low temperature have better performance comparing with other samples aged at normal temperature, the flexible vibration peak of S=O bond has been strengthened remarkably in IR spectra. The peak position of W4f have a higher chemical shift in XPS patterns. The diffraction peaks of tetragonal and orthographic phase of WO3 are stronger in XRD patterns. The process of ageing at low temperature is responsible for the stronger acidity and higher activity of SWT samples. 展开更多
关键词 固体超强酸催化剂 低温陈化法 制备 氧化钨 二氧化钛 催化性能
下载PDF
V(Ⅴ)促进SO_4^(2-)/ZrO_2固体超强酸的制备及催化反应 被引量:13
2
作者 郑明东 陈同云 胡克良 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2006年第6期1086-1090,共5页
用低温陈化的方法制得V(Ⅴ)促进型SO42-/ZrO2固体超强酸(SZV),用流动指示剂法测定其酸强度,用IR,XRD和XPS进行结构表征,并将制得的催化剂用于催化乙酸和丙三醇的酯化反应.结果表明,低温陈化样品比常温陈化有更强的酸性和更高的催化活性... 用低温陈化的方法制得V(Ⅴ)促进型SO42-/ZrO2固体超强酸(SZV),用流动指示剂法测定其酸强度,用IR,XRD和XPS进行结构表征,并将制得的催化剂用于催化乙酸和丙三醇的酯化反应.结果表明,低温陈化样品比常温陈化有更强的酸性和更高的催化活性,IR谱图中S O键的伸缩振动峰显著增强,在600~650℃的焙烧温度下,低温陈化样品的晶体结构为ZrO2四方相,XPS图中Zr3d峰位出现较大的化学位移,表明低温陈化使SZV样品具有较高的酸性. 展开更多
关键词 低温陈化 固体超强酸 制备 酯化反应 三醋酸甘油酯