Friction-reducing and antiwear behavior of metal halide-stabilized linear phosphazene derivatives as lubricants for a steel-on-steel contact
1
作者 ZHU Jiamei 1,2 , LIU Weimin 2 & LIANG Yongmin 2 1. School of Chemical Engineering and Technology, China University of Mining and Technology, Xuzhou 221008, China 2. State Key Laboratory of Solid Lubrication, Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences, Lanzhou 730000, China 《Science China(Technological Sciences)》 SCIE EI CAS 2005年第3期282-291,共10页
A series of novel metal halide-stabilized linear phosphazene derivatives were synthesized. The friction-reducing and antiwear abilities of the resulting products as the lubricants for a steel-on-steel contact were com... A series of novel metal halide-stabilized linear phosphazene derivatives were synthesized. The friction-reducing and antiwear abilities of the resulting products as the lubricants for a steel-on-steel contact were comparatively investigated on an Optimol SRV oscillating friction and wear tester. The morphology of the worn steel surface was observed on a scanning electron microscope, while the chemical states of some typical elements on the worn steel surface were examined by means of X-ray photoelectron spectroscopy. It was found that both the side branch structures and central metals influenced the friction-reducing and antiwear behaviors of the synthetic derivatives as the lubricants, which was related to the different adsorption activities of the organic compounds composed of different organic ingredients and metallic ions on a nascent metal surface. All the synthetic lubricants except for the iron (III) derivative showed increased antiwear abilities with increasing metallic ionic radius. A protective layer originated from the tribochemical reaction together with the adsorbed boundary lubricating layer containing organic fluorine compounds, nitrogen oxide, and Fe 3 (PO 4 ) 2 plays an important role in improving the friction and wear behavior of the steel-on-steel system. 展开更多
关键词 metal halide-stabilized LINEAR PHOSPHAZENE derivatives lubricant steel tribological properties.
原文传递
照相稳定剂583对扁平卤化银乳剂微晶的增感作用 被引量:4
2
作者 王荣琴 杨赣 《感光材料》 北大核心 1997年第3期21-24,共4页
应用双注仪制备了单分散六边形扁平溴碘化银乳剂微晶,研究了照相稳定剂583对乳剂照相性能和电性质的影响。结果表明:583对S+Au增感的扁平溴碘化银乳剂微晶有明显的增感作用,而对未经化学增感的乳剂没有增感作用。从583... 应用双注仪制备了单分散六边形扁平溴碘化银乳剂微晶,研究了照相稳定剂583对乳剂照相性能和电性质的影响。结果表明:583对S+Au增感的扁平溴碘化银乳剂微晶有明显的增感作用,而对未经化学增感的乳剂没有增感作用。从583对离子过程、电子的复合和捕获过程的影响进一步研究了其增感机理。 展开更多
关键词 稳定剂583 增感机理 卤化银乳剂 照相乳剂
下载PDF
无机卤化物对不溶性硫稳定性的影响 被引量:5
3
作者 武文良 王勇 +2 位作者 曾崇余 汪雄辉 周立进 《高校化学工程学报》 EI CAS CSCD 北大核心 2006年第3期356-361,共6页
在液相法制备不溶性硫(IS)的过程中,以无机卤化物KCl、KBr、KI作为稳定剂,采用单因素法确定了适宜的稳定剂用量、反应温度和反应时间。实验结果表明,稳定剂KCl的适宜用量为0.6%,反应时间1h,反应温度260℃,IS收率为17.09%;稳定剂KBr适宜... 在液相法制备不溶性硫(IS)的过程中,以无机卤化物KCl、KBr、KI作为稳定剂,采用单因素法确定了适宜的稳定剂用量、反应温度和反应时间。实验结果表明,稳定剂KCl的适宜用量为0.6%,反应时间1h,反应温度260℃,IS收率为17.09%;稳定剂KBr适宜用量为0.8%,反应时间90min,反应温度280℃,IS收率为28.5%;稳定剂KI适宜用量为0.6%,反应时间1h,反应温度240℃,IS收率为29.30%。在研究IS热稳定性的过程中,对用三种稳定剂所制备的IS进行充环烷油、脂肪烃油、芳烃油处理,比较了工艺油的品种和稳定剂的协同作用对IS的受热影响。在105℃下15min内,三种工艺油中,以IS充芳烃油的热稳定性为最高;三种稳定剂中,以KI制备的IS充油后的热稳定性最好;以KCl、KBr、KI为稳定剂所制备的IS充芳烃油的热稳定性顺序依次为76.3%、87.5%、96.0%,同时初步讨论了工艺油种类和无机卤化物对抑制IS还原的作用机理。 展开更多
关键词 卤化物稳定剂 不溶性硫 热稳定性 工艺油
下载PDF