Amorphous porous carbon was synthesized by chemical vapor deposition on copper substrates. The average size of the pores is around 1.2 microns with some small pores decorating the big ones. Lamellar samples of this ca...Amorphous porous carbon was synthesized by chemical vapor deposition on copper substrates. The average size of the pores is around 1.2 microns with some small pores decorating the big ones. Lamellar samples of this carbonaceous material can be separated from the copper support and may be useful as electrode due to its low electrical resistivity of the order of 0.4 Ωcm.展开更多
文摘Amorphous porous carbon was synthesized by chemical vapor deposition on copper substrates. The average size of the pores is around 1.2 microns with some small pores decorating the big ones. Lamellar samples of this carbonaceous material can be separated from the copper support and may be useful as electrode due to its low electrical resistivity of the order of 0.4 Ωcm.