Comprehensive Utilization of Paigeite Ore Using Iron Nugget Making Process 被引量:18
1
作者 DING Yin-gui WANG Jing-song +2 位作者 WANG Guang MA Sai XUE Qing-guo 《Journal of Iron and Steel Research International》 SCIE CAS CSCD 2012年第6期9-13,共5页
The feasibility of paigeite ore treatment with iron nugget making process is proved. The isothermal reduc- tion experiments at laboratory scale were carried out, using carbon bearing pellets which were made of boron c... The feasibility of paigeite ore treatment with iron nugget making process is proved. The isothermal reduc- tion experiments at laboratory scale were carried out, using carbon bearing pellets which were made of boron contai- ning iron concentrate and pulverized coal mainly, from 1 623 to 1 723 K with different heating time. The results indi- cated that iron nugget making process depends mainly on heating time and temperature. And the iron nugget and slag can separate in a clean manner at 1 673 K for 15 min. For the iron nugget, the C content is 3.57% (mass percent) and B is 0. 065~ (mass percent). The B203 content of slag is 20.01~/00, and the boron was concentrated into one phase which is identified as suanite (Mg2BaOs) during the solidification. With an extraction ratio of 80~ under the atmospheric conditions, the activity of boron in slag is good. The boron-rich slag can be used to extract boric or boric acid and alleviate the shortage of boron resource. Through series of calculation and analysis related, it can be conclu- ded that the recovery ratio of Fe and boron are about 98% and 97% respectively. The results show that this method is feasible and effective on the utilization of paigeite ore. 展开更多
关键词 boron containing iron concentrate carbon bearing pellets iron nugget boron-rich slag
原文传递
含硼铁精矿粉/环氧树脂复合材料射线屏蔽性能研究 被引量:9
2
作者 李哲夫 薛向欣 姜涛 《功能材料》 EI CAS CSCD 北大核心 2010年第11期1892-1895,共4页
以我国特有的含硼矿物经选矿后得到的含硼铁精矿粉作为中子吸收体与低粘度环氧树脂E51相复合,制备了一种低成本含硼铁精矿粉/环氧树脂复合屏蔽材料。测试了这种复合材料对慢中子和60Coγ射线的屏蔽性能,确定了满足射线屏蔽性能的含硼铁... 以我国特有的含硼矿物经选矿后得到的含硼铁精矿粉作为中子吸收体与低粘度环氧树脂E51相复合,制备了一种低成本含硼铁精矿粉/环氧树脂复合屏蔽材料。测试了这种复合材料对慢中子和60Coγ射线的屏蔽性能,确定了满足射线屏蔽性能的含硼铁精矿粉与树脂的最佳配比范围。证明了以含硼铁精矿粉作为原料制备复合射线屏蔽材料是可行的。结果表明,3种配比的复合屏蔽材料其慢中子宏观截面均超过了宏观截面为Σ=0.158cm-1,以B4C为中子吸收体的铅硼聚乙烯屏蔽材料B201。此复合屏蔽材料的宏观截面最大值为Σ=0.1882cm-1,具备较好的慢中子屏蔽能力;对60Coγ射线的线性减弱系数最大值为μ=0.0772cm-1,屏蔽性能介于水和混凝土之间。 展开更多
关键词 含硼铁精矿粉 环氧树脂 低成本 慢中子 ^60Coγ射线 屏蔽材料