Pretreatment and thiosulfate leaching of refractory gold-bearing arsenosulfide concentrates 被引量:6
1
作者 Yuqun Meng 《Journal of University of Science and Technology Beijing》 CSCD 2005年第5期385-389,共5页
A hydrometallurgical process for refractory gold-bearing arsenosulfide concentrates at ambient temperature and pressure was presented, including fine grinding with intensified alkali-leaching (FGIAL), enhanced agita... A hydrometallurgical process for refractory gold-bearing arsenosulfide concentrates at ambient temperature and pressure was presented, including fine grinding with intensified alkali-leaching (FGIAL), enhanced agitation alkali-leaching (EAAL), thiosulfate leaching and displacement. Experimental results on a refractory gold concentrate showed that the total consumption of NaOH in alkaline leaching is only 41% of those theoretically calculated under the conditions of full oxidization for the same amount of arse- nides and sulfides transformed into arsenates and sulfates, and 72.3% of gold is synchro-dissoluted by thiosulfate self-generated during alkaline leaching. After alkaline leaching, thiosulfate leaching was carried out for 24 h. The dissolution of gold is increased to 91.9% from 4.6% by cyanide without the pretreatment. The displacement of gold by zinc powder in the solution gets to 99.2%. Due to an amount of thiosulfate self-generated during alkaline leaching, the reagent addition in thiosulfate leaching afterwards is lower than the normal. 展开更多
关键词 refractory gold-bearing arsenosulfide concentrates PRETREATMENT alkaline leaching self-leaching of gold thiosulfate leaching
下载PDF
A new extraction process of refractory gold arsenosulfide concentrates 被引量:3
2
作者 YuqunMeng TaoJin +2 位作者 MinjieWu ShaolingSu LongbaoWang 《Journal of University of Science and Technology Beijing》 CSCD 2003年第5期9-14,共6页
A new hydrometallurgical process for the refractory gold arsenosulfideconcentrates under normal temperature and pressure was presented. The experimental results of arefractory gold concentrate show that the total cons... A new hydrometallurgical process for the refractory gold arsenosulfideconcentrates under normal temperature and pressure was presented. The experimental results of arefractory gold concentrate show that the total consumption of NaOH in alkaline leaching is only 40%of those theoretically calculated under the conditions of full oxidization at the same oxidation ofarsenic to ar-senate and sulfur to sulfate. After alkaline leaching, cyanidation and adsorptionwere carried out for 24 h. The dissolution of gold by NaCN is increased to 95.3% from 12.8% beforepretreatment, and meanwhile 99.3% of the adsorption of gold by activated charcoal. The consumptionof NaCN for one ton ore is 10 kg, which is 1.2 times less than that before pretreatment. As it iscarried out under normal temperature and pressure, the investment of installations is alsodecreased. 展开更多
关键词 refractory gold arsenosulfide concentrates normal temperature and pressure PRETREATMENT
下载PDF
难浸砷金精矿的碱性常温常压预氧化 被引量:14
3
作者 孟宇群 《贵金属》 CAS CSCD 2004年第3期1-5,共5页
本文提供了1种难浸金精矿的湿法预氧化新工艺,它包括细磨、强化碱浸预氧化、氰化和炭吸附。在螺旋搅拌式塔式磨浸机中,先将目的难浸金精矿细磨至98%<37μm,然后在40%的矿浆质量浓度、11℃的环境温度和0.1MPa的环境压力下强化碱浸24h,... 本文提供了1种难浸金精矿的湿法预氧化新工艺,它包括细磨、强化碱浸预氧化、氰化和炭吸附。在螺旋搅拌式塔式磨浸机中,先将目的难浸金精矿细磨至98%<37μm,然后在40%的矿浆质量浓度、11℃的环境温度和0.1MPa的环境压力下强化碱浸24h,NaOH的消耗量为88kg/t矿,仅为相同氧化率条件下将砷硫氧化成砷酸盐和硫酸盐所需理论碱耗量的30%。预氧化完成后经36h的氰化浸出和炭吸附,金的浸出率从预氧化前的24.6%提高到95.4%,金的吸附率99.2%,NaCN的消耗4kg/t矿。整个提金工艺的成本约300元/t矿。 展开更多
关键词 难浸砷金精矿 预氧化 常温常压 冶金原料 细磨 碱浸 氰化 炭吸附
下载PDF
某含砷金矿石提高回收率研究 被引量:16
4
作者 孟宇群 代淑娟 宿少玲 《黄金》 CAS 北大核心 2005年第1期34-36,共3页
采用塔式磨浸机细磨和碱浸预处理工艺 ,在磨矿细度 - 40 0目粒级质量分数为 95 % ,4 0 %的矿浆浓度和 8.5℃的环境温度下 ,使用NaOH和CaO对砷质量分数为 2 %的金矿石碱浸预处理 16h ,金的氰化浸出率从细磨碱浸前的 75 .6 %提高到 93.3%... 采用塔式磨浸机细磨和碱浸预处理工艺 ,在磨矿细度 - 40 0目粒级质量分数为 95 % ,4 0 %的矿浆浓度和 8.5℃的环境温度下 ,使用NaOH和CaO对砷质量分数为 2 %的金矿石碱浸预处理 16h ,金的氰化浸出率从细磨碱浸前的 75 .6 %提高到 93.3%。细磨和碱浸预处理成本大约 12 6元 /t。采用该技术对 5 0t/d规模的某黄金冶炼厂进行改造 ,每年可以多回收黄金 4 3.5kg ,3个半月收回细磨和预处理系统的设备投资。 展开更多
关键词 含砷金矿石 细磨 碱浸预处理 提高回收率
下载PDF
某含砷金矿石选冶技术研究与应用 被引量:1
5
作者 徐世杰 宋建斌 《中国矿山工程》 2006年第3期17-18,25,共3页
某金矿采用浮选—精矿加压碱法预氧化—氰化提金工艺取代原矿加压碱法预氧化—氰化提金工艺,仅增加一套浮选设备,使金回收率由原来60%提高到81%,年可多回收黄金32kg,创造效益213万元。