Anti-catalytic and zincophilic layers integrated zinc anode towards efficient aqueous batteries for ultra-long cycling stability 被引量:4
1
作者 Chunli Wang Yuxing Gao +6 位作者 Lianshan Sun Yuan Zhao Dongming Yin Hairui Wang Jingchao Cao Yong Cheng Limin Wang 《Nano Research》 SCIE EI CSCD 2022年第9期8076-8082,共7页
Aqueous zinc-based battery is usually plagued by serious dendrites and side reactions including Zn corrosion and water decomposition on the anode.To address the drawbacks,constructing coating layers with high conducti... Aqueous zinc-based battery is usually plagued by serious dendrites and side reactions including Zn corrosion and water decomposition on the anode.To address the drawbacks,constructing coating layers with high conductivity and anti-catalytic effects on hydrogen evolution reaction has been considered as an efficient strategy.Herein,cheap and abundant twodimensional(2D)conductive graphite(KS-6)coating layer with high electronic conductivity(~106 S·m^(−1))could directly form strong bonding with Zn foil due to high zincophilicity,which correspondingly protects Zn metal from liquid electrolyte to inhibit parasitic hydrogen evolution and guide uniform Zn electrodeposition during cycling.The KS-6 layer owns a profitable charge redistribution effect to endow Zn anode with a lower nucleation energy barrier and a more uniformly distributed electric field compared with bare Zn.Therefore,such integrated Zn anode exhibits low voltage hysteresis(~38 mV)and excellent cycling stability with dendrite-free behaviors(1 mA·cm^(−2)and 2 mAh·cm^(−2))over 2,000 h,far outperforming many reported Zn metal anodes in aqueous systems.Encouragingly,in light of the superior Zn@KS-6 anode,VNOx powders and Prussian blue analogs Mn_(2)Fe(CN)_(6)are applied as the cathode materials to assemble full batteries,which show remarkable cycling stabilities and high Coulombic efficiencies(CEs)over 200 cycles with capacity retention of 81.5%for VNOx//Zn@KS-6 battery and over 400 cycles with capacity retention of 94.6%for Mn_(2)Fe(CN)_(6)//Zn@KS-6 battery,respectively. 展开更多
关键词 aqueous battery zinc-dendrite anti-catalysis zincophilicity two-dimensional(2D)conductive graphite
原文传递
铜的反催化分光光度法——铜(Ⅱ)-过硫酸钾-甲基红体系 被引量:14
2
作者 万全玉 汪敬武 张振辉 《分析化学》 SCIE EI CAS CSCD 北大核心 1993年第2期215-217,共3页
本文提出一种利用铜在乙醇介质中阻抑过硫酸钾氧化甲基红来测定痕量铜的新方法。采用动力学光度法可测定低至0.4ng/ml Cu^(2+)。本法用于水和试剂中的测定,结果令人满意。
关键词 反催化 分光光度法
下载PDF
反催化分光光度法测定痕量铬(Ⅵ)的研究 被引量:3
3
作者 吴宪龙 《化学研究与应用》 CAS CSCD 1997年第5期504-506,共3页
反催化分光光度法测定痕量铬(Ⅵ)的研究吴宪龙(辽宁工学院化工系锦州121001)关键词铬反催化分光光度法中图分类号O657.32铬(Ⅵ)是世界各国环境监测必测元素之一。对痕量铬(Ⅵ)测定方法的研究一直是人们关注的课题... 反催化分光光度法测定痕量铬(Ⅵ)的研究吴宪龙(辽宁工学院化工系锦州121001)关键词铬反催化分光光度法中图分类号O657.32铬(Ⅵ)是世界各国环境监测必测元素之一。对痕量铬(Ⅵ)测定方法的研究一直是人们关注的课题。近年来在催化动力学分析方法的研究... 展开更多