V_2O_5-WO_3-MoO_3/TiO_2催化剂在柴油机NH_3-SCR系统中的性能 被引量:7
1
作者 高岩 栾涛 +1 位作者 彭吉伟 XU Hongming 《化工学报》 EI CAS CSCD 北大核心 2013年第9期3356-3366,共11页
针对柴油机运行工况特点及柴油机尾气成分特点,以工业纯锐钛型二氧化钛、偏钒酸铵、偏钨酸铵、钼酸铵为主要原料制备了颗粒状V2O5-WO3-MoO3/TiO2催化剂,以Lister Petter TR1重型直喷式单缸柴油机为依托搭建试验台,研究了在真实柴油机尾... 针对柴油机运行工况特点及柴油机尾气成分特点,以工业纯锐钛型二氧化钛、偏钒酸铵、偏钨酸铵、钼酸铵为主要原料制备了颗粒状V2O5-WO3-MoO3/TiO2催化剂,以Lister Petter TR1重型直喷式单缸柴油机为依托搭建试验台,研究了在真实柴油机尾气环境下催化剂的脱硝性能。结果表明,柴油机负载增大,催化剂脱硝活性呈现下降趋势。1800r·min-1时,脱硝活性最大值87.1%在负载25%、反应温度380℃、空速20000h-1、氨氮比1.0处取得。柴油机负载不同,导致催化剂活性温度窗口(脱硝活性>70%)发生较大变化,与负载25%相比,负载50%活性温度窗口减小约60℃。增大柴油机负载可以提高NH3/N2O反应起始温度,但是同时会导致高温区间(>400℃)N2O生成量增大。 展开更多
关键词 SCR NH3 Nox v2o5-wo3-moo3 Tio2 柴油机
下载PDF
选择性催化还原蜂窝状催化剂工业试验研究 被引量:44
2
作者 高岩 栾涛 +2 位作者 程凯 吕涛 郑衍娟 《中国电机工程学报》 EI CSCD 北大核心 2011年第35期21-28,0+8,共8页
以工业级药品为主要成分,制备选择性催化还原(selective catalytic reduction,SCR)蜂窝状催化剂,利用工业试验台对其活性进行测试,取得了催化剂在真实烟气情况下,不同空速、催化剂用量、温度、氨氮比、NOx初始浓度等因素对催化剂活性的... 以工业级药品为主要成分,制备选择性催化还原(selective catalytic reduction,SCR)蜂窝状催化剂,利用工业试验台对其活性进行测试,取得了催化剂在真实烟气情况下,不同空速、催化剂用量、温度、氨氮比、NOx初始浓度等因素对催化剂活性的作用效果。文中真实烟气环境下SCR脱硝系统运行存在最佳工况范围:SCR反应塔入口温度360~390℃,出口温度330~360℃,氨氮比为0.85~1,空速在4000~6000h-1。此工况下,催化剂脱硝效率可以达到84%。催化剂的75%活性温度窗口为320~400℃,且峰值在380℃处取得。催化剂的脱硝效率随氨氮比变化明显,当氨氮比达到0.9时,催化剂脱硝效率超过80%。催化剂对NOx浓度适应性较好,NOx初始浓度在615~3485mg·m-3范围内,催化剂的脱硝效率始终保持在70%以上。 展开更多
关键词 蜂窝状催化剂 选择性催化还原 真实烟气 影响因素v2o5-wo3-moo3/Tio2
下载PDF
Performance of V_2O_5-WO_3-MoO_3/TiO_2 Catalyst for Selective Catalytic Reduction of NO_x by NH_3 被引量:9
3
作者 高岩 栾涛 +2 位作者 吕涛 程凯 徐宏明 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2013年第1期1-7,共7页
The V/O5-WO3-MoOy'TiO2 honeycomb catalyst was prepared with industrial grade chemicals. The structural and physico-chemical properties were analyzed with X-ray diffraction (XRD), scanning electron micrograph (SEM... The V/O5-WO3-MoOy'TiO2 honeycomb catalyst was prepared with industrial grade chemicals. The structural and physico-chemical properties were analyzed with X-ray diffraction (XRD), scanning electron micrograph (SEM) and mercury porosimetry. The NOx conversion and durability were investigated on a pilot plant test set under the actual operational conditions of a coal fired boiler. The catalyst monolith had good formability with mass per- centage of V : W : Mo : TiO2 : fiber glass = 1 : 4.5 : 4.5 : 72 : 18. Vanadium, tungsten and molybdenum species were highly dispersed on anatase TiO2 without causing the transformation of anatase TiO2 to ruffle by calcining under a current of air at 450℃ for 4.5 h, but there were some degrees of crystal distortion. The catalyst particle sizes were almost uniform with close pile-up and the pore structure was regular with complete macro-pore formation and large specific surface area. The NOx conversion was sensitive to temperature but nearly insensitive to NH3. The catalyst showed strong adaptability to NOx concentration with activity above 80% in the range of 615 1640 mg.m-3. Within the range of 720-8640 h continuous operation, the NOx conversion dropped at a rate of about 1% reduction per 600 h. 展开更多
关键词 selective catalytic reduction v2o5-wo3-moo3/Zio2 catalyst physico-chemical property flue gas life time
下载PDF
一种新型SCR烟气脱硝催化剂的研究 被引量:2
4
作者 董月红 薛洋企 李兵 《电力科技与环保》 2015年第6期28-31,共4页
以二氧化钛、硅铝纤维纸为载体,通过浸渍法制备了一种新型的V_2O_5-WO_3-MoO_3/TiO_2催化剂。对催化剂进行SEM、XRD、N_2吸附等表征分析和脱硝活性测试,结果表明,在载体及催化剂的制备过程中,煅烧温度均为500℃,载体和催化剂均能保持较... 以二氧化钛、硅铝纤维纸为载体,通过浸渍法制备了一种新型的V_2O_5-WO_3-MoO_3/TiO_2催化剂。对催化剂进行SEM、XRD、N_2吸附等表征分析和脱硝活性测试,结果表明,在载体及催化剂的制备过程中,煅烧温度均为500℃,载体和催化剂均能保持较好的多孔性质,同时锐钛矿TiO_2未金红石化;当催化剂活性成分V_2O_5、WO_3,MoO_3质量分数分别为3%、7%、4%时,在模拟烟气条件下其脱硝效率可达92%。 展开更多
关键词 SCR v2o5-wo3-moo3/Tio2 催化剂载体 脱硝效率