Using free bending method,the residual stress of the Ti(CN)coating on alloy Nb-752 was measured to be 2-3 GPa of which the thermal stress cmounts to 10—20%.An analysis on coating/substrate interface stress state show...Using free bending method,the residual stress of the Ti(CN)coating on alloy Nb-752 was measured to be 2-3 GPa of which the thermal stress cmounts to 10—20%.An analysis on coating/substrate interface stress state shows that the share stress at it is about O.1—0.2 GPa.The demage mode of the coating under external loading was proposed in terms of the amount and the direction of loading.展开更多
文摘Using free bending method,the residual stress of the Ti(CN)coating on alloy Nb-752 was measured to be 2-3 GPa of which the thermal stress cmounts to 10—20%.An analysis on coating/substrate interface stress state shows that the share stress at it is about O.1—0.2 GPa.The demage mode of the coating under external loading was proposed in terms of the amount and the direction of loading.