单分散蛋黄状SiO_2/TiO_2球的制备及其电流变性能
1
作者 陈雨露 李冬 +2 位作者 苏明 郭小松 郝春成 《青岛科技大学学报(自然科学版)》 CAS 2017年第2期71-77,共7页
以SiO_2为模板,钛酸丁酯为钛源,NaOH为刻蚀剂,模板法结合溶胶凝胶法及部分刻蚀工艺成功制备了单分散蛋黄状SiO_2/TiO_2核壳复合微球,并以其作为电流变液的分散相材料研究分散相颗粒结构的转变对电流变性能的影响。通过X-射线衍射仪,扫... 以SiO_2为模板,钛酸丁酯为钛源,NaOH为刻蚀剂,模板法结合溶胶凝胶法及部分刻蚀工艺成功制备了单分散蛋黄状SiO_2/TiO_2核壳复合微球,并以其作为电流变液的分散相材料研究分散相颗粒结构的转变对电流变性能的影响。通过X-射线衍射仪,扫描电子显微镜和透射电子显微镜表征手段,探讨了蛋黄状SiO_2/TiO_2核壳复合微球的逐步形成过程。电流变测试结果表明,蛋黄状SiO_2/TiO_2电流变液的电流变效应随着SiO_2内核尺寸的减小而提高,这主要是由密度变小的分散相颗粒在电场中提高的电场力所致。详细探讨了分散相颗粒密度,沉降稳定性与电流变性能三者之间的关系。结果发现:分散相颗粒密度越低,沉降稳定性越好,电流变性能更佳。 展开更多
关键词 sio2/tio2微球 蛋黄结构 电流变性能 抗沉降性
下载PDF
Photodegradation of Binary Azo Dyes Using Core-Shell Fe<sub>3</sub>O<sub>4</sub>/SiO<sub>2</sub>/TiO<sub>2</sub>Nanospheres
2
作者 Eman Alzahrani 《American Journal of Analytical Chemistry》 2017年第1期95-115,共21页
Photodegradation has emerged as an environmentally friendly method of decomposing harmful dyes in wastewater. In this study, core-shell Fe3O4/SiO2/ TiO2 nanospheres with magnetic cores were obtained from synthesised m... Photodegradation has emerged as an environmentally friendly method of decomposing harmful dyes in wastewater. In this study, core-shell Fe3O4/SiO2/ TiO2 nanospheres with magnetic cores were obtained from synthesised magnetic Fe3O4 nanoparticles through the precipitation method, the surface of the magnetic Fe3O4 nanoparticles was coated with a silica (SiO2) layer by hydrolysis of tetramethoxysilane (TMOS) as a silica source, and finally, Fe3O4/SiO2 nanospheres were coated with titanium (TiO2) layer using tetrabutyltitanate (TBT) as a precursor through the sol-gel process. The morphology and structure of the prepared materials were characterised by X-ray diffraction (XRD) analysis, scanning electron microscopy (SEM), X-ray energy dispersive spectrometry (EDAX), Fourier transform infrared spectroscopy (FT-IR), and atomic force microscopy (AFM). The photocatalytic activities of the prepared core-shell nanospheres were studied using binary azo dyes, namely methyl orange (anionic dye, MO) and methylene blue (cationic dye, MB) in aqueous solution under UV light irradiation (365 nm), and UV-Vis spectrophotometer was utilised to monitor the amount of each dye in the mixture. It was found that 90.2% and 100% of binary MO and MB were removed for 5 h, respectively. The results revealed that the efficiency of the photocatalytic degradation of the core-shell nanospheres was not degreased after five runs that can be used as recyclable photocatalysts. The results show that the performance of the prepared core-shell nanospheres was better than that of commercial TiO2 nanoparticles. Moreover, the magnetic separation properties of the core-shell Fe3O4/SiO2/TiO2 nanospheres can enable the prepared materials to have wider application prospects. 展开更多
关键词 Fe3O4/sio2/tio2 nanospheres CORE-SHELL Magnetic Photocatalyst Sol-Gel Method BINARY Azo Dyes PHOTODEGRADAtioN
下载PDF
蒸汽相水解法制备磁性光催化剂Fe_3O_4/SiO_2/TiO_2及其光催化性能 被引量:2
3
作者 郭冬雪 宗海伦 +1 位作者 吴一泓 张青红 《中国科技论文》 CAS 北大核心 2014年第6期637-641,共5页
采用蒸汽相水解法,以Fe3O4纳米磁性颗粒为磁核,在其表面包覆一层SiO2来阻止光腐蚀,然后将锐钛矿相纳米氧化钛沉积在Fe3O4/SiO2颗粒表面,从而制得核壳结构的Fe3O4/SiO2/TiO2磁性复合光催化材料。用X射线粉末衍射仪(XRD)、场发射扫描电镜(... 采用蒸汽相水解法,以Fe3O4纳米磁性颗粒为磁核,在其表面包覆一层SiO2来阻止光腐蚀,然后将锐钛矿相纳米氧化钛沉积在Fe3O4/SiO2颗粒表面,从而制得核壳结构的Fe3O4/SiO2/TiO2磁性复合光催化材料。用X射线粉末衍射仪(XRD)、场发射扫描电镜(FE-SEM)、高分辨率透射电子显微镜(HR-TEM)、探针式震动磁强计等手段对所制备的产物的结构、形貌、磁强度性能进行表征。以300W汞灯为光源,用亚甲基蓝和酸性红模拟污水中的有机染料来评价复合光催化剂的性能。结果表明,磁性纳米微球中TiO2的含量越大,其光催化性能越好,含TiO2质量分数50%的F3O4/SiO2/TiO2磁性纳米微球可在180min内降解亚甲基蓝模拟染料废水,降解率达99%,在80min内降解酸性模拟染料废水,降解率达98%。 展开更多