Two sapphire substrates were tightly bonded by irradiation with a 1064 nm nanosecond laser and using a sputtered 50 nm-titanium thin film as an absorbing medium.Upon laser irradiation,aluminum from the upper substrate...Two sapphire substrates were tightly bonded by irradiation with a 1064 nm nanosecond laser and using a sputtered 50 nm-titanium thin film as an absorbing medium.Upon laser irradiation,aluminum from the upper substrate is incorporated into the thin film,forming Ti-Al-O compounds.While the irradiated region becomes transparent,the bond quality was evaluated by scanning acoustic microscopy.展开更多
基金financial support of FhG Internal Programs(Grant No.692 280)
文摘Two sapphire substrates were tightly bonded by irradiation with a 1064 nm nanosecond laser and using a sputtered 50 nm-titanium thin film as an absorbing medium.Upon laser irradiation,aluminum from the upper substrate is incorporated into the thin film,forming Ti-Al-O compounds.While the irradiated region becomes transparent,the bond quality was evaluated by scanning acoustic microscopy.