作者 贾继飞 沈俭一 +3 位作者 徐竹生 葛欣 张涛 林励吾 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 1997年第6期958-960,共3页
The reduction behavior of Y-Al2O3 supported iron and platinum-iron catalysts was studied by TPR combined in situ 57Fe MBS. The results indicated that Fe3+ is highly dis-persed on the Y-Al2O3 surface for all the sample... The reduction behavior of Y-Al2O3 supported iron and platinum-iron catalysts was studied by TPR combined in situ 57Fe MBS. The results indicated that Fe3+ is highly dis-persed on the Y-Al2O3 surface for all the samples containing iron before the reduction. No Fe was found in the reduction process. The Fe3+ was reduced to Fe2+ in tetrahedral vacancy first in Pt-Fe/Y-Al2O3 sample in TPR process. The TPR processes of all supported iron samples are very different from those of α-Fe2O3. 展开更多
关键词 催化剂 表面结构 γ三氧化二铝 TPR MBS
下载PDF
介孔Pt-Fe/Al_(2)O_(3)强化类芬顿催化降解罗丹明B性能与机理
2
作者 蒲浩 王雁 +2 位作者 郭泽宇 胡干琳 赵旭 《环境科学学报》 CAS CSCD 北大核心 2024年第7期83-94,共12页
以蒸发诱导自组装法制备了介孔氧化铝载体,然后通过浸渍法制备了Pt-Fe/Al_(2)O_(3)异相类芬顿催化剂,制备的Pt-Fe/Al_(2)O_(3)催化剂可高效活化H_(2)O_(2)氧化降解有机污染物.首先对比了国内外不同厂家生产的造孔剂P123对氧化铝载体比... 以蒸发诱导自组装法制备了介孔氧化铝载体,然后通过浸渍法制备了Pt-Fe/Al_(2)O_(3)异相类芬顿催化剂,制备的Pt-Fe/Al_(2)O_(3)催化剂可高效活化H_(2)O_(2)氧化降解有机污染物.首先对比了国内外不同厂家生产的造孔剂P123对氧化铝载体比表面积和物相结构的影响,进而表征了Pt-Fe/Al_(2)O_(3)的理化结构与催化性能.结果表明,在0.2 g·L^(-1)Pt-Fe/Al_(2)O_(3)、p H=3、H_(2)O_(2)浓度为10 mmol·L^(-1)的条件下,所制备催化剂在30 min内对20 mg·L^(-1)罗丹明B(Rh B)溶液的降解效率达到97.71%.介孔Pt-Fe/Al_(2)O_(3)具有较好的循环使用稳定性,并对Rh B、甲基橙(MO)、亚甲基蓝(MBT)等多种有机污染物均具有良好的降解效果,是一种有前景的异相类芬顿催化剂.猝灭实验和ESR结果表明,·OH和^(1)O_(2)是Rh B降解的主要活性物种. 展开更多
关键词 类芬顿催化 介孔氧化铝 pt-fe/al_(2)o_(3) 罗丹明B 降解
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部