Characterization of Interfacial Bonding Mechanism for Graphene-Modified Powder Metallurgy Nickle-Based Superalloy
1
作者 Jin-Wen Zou Xiao-Feng Wang +4 位作者 Jie Yang Chuan-Bo Ji Xu-Qing Wang Xian-Qiang Fan Zhi-Peng Guo 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2018年第7期753-760,共8页
A modified FGH96 superalloy using 0.1 wt% graphene was successfully prepared using the wet mixing method. The interracial bonding mechanism between the graphene and the superalloy matrix was characterized using optica... A modified FGH96 superalloy using 0.1 wt% graphene was successfully prepared using the wet mixing method. The interracial bonding mechanism between the graphene and the superalloy matrix was characterized using optical micro- scope, scanning electronic microscope, transmission electronic microscope and X-ray tomography. The results revealed that the graphene could be dispersed uniformly inside the matrix of the superalloy, and the bonding interface between graphene and the superalloy showed a rather diffusion instead of abrupt distinction, suggesting that the interface was formed via chemical fusion rather than a mechanical combination. The uniform dispersity of the graphene inside the superalloy matrix could improve the tensile properties significantly, including tensile strength, plasticity and yield strength. The existence of the graphene at the fracture surface further verified that the graphene could increase the effective bearing force of the material during the tensile test. 展开更多
关键词 powder metallurgicalpmsuperalloy GRAPHENE Interfacial binding mechanism Mechanical propertiesCharacterization
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部