Novel potassium ion selective electrodes (K^+ISEs) and cDNA array sensors based on porous silicon (PS) have been developed.The calibration curve for the K^+ISEs is linear within a wide range of pK=2.0~6.0 with the sl...Novel potassium ion selective electrodes (K^+ISEs) and cDNA array sensors based on porous silicon (PS) have been developed.The calibration curve for the K^+ISEs is linear within a wide range of pK=2.0~6.0 with the slope of 56 mV per decade,which is near Nernst response.The response time and detection limit are within 31 s and 0.5μmol/L,respectively.The selective coefficient for Na^+ is-3.8,satisfies the requirement for the assay of blood potassium.The response variation is within 2 mV during 2 months.The binding capacity,the dynamic range and the detection limit of the DNA sensors were improved by replacing glass slide with PS substrates.The cDNA array sensors can bear 80℃of high temperature,75% of humidity,3.6 kLx of irradiation and keep stable within 10 days when they are exposed in air.Good performances of the K^+ISE and the cDNA array sensor are attributed to the large internal surface area and the easily modified microstructure of PS.展开更多
基金supported by National Natural Science Foundation of China(69925409,60276036)Shanghai Applied Material Foundation(0202).
文摘Novel potassium ion selective electrodes (K^+ISEs) and cDNA array sensors based on porous silicon (PS) have been developed.The calibration curve for the K^+ISEs is linear within a wide range of pK=2.0~6.0 with the slope of 56 mV per decade,which is near Nernst response.The response time and detection limit are within 31 s and 0.5μmol/L,respectively.The selective coefficient for Na^+ is-3.8,satisfies the requirement for the assay of blood potassium.The response variation is within 2 mV during 2 months.The binding capacity,the dynamic range and the detection limit of the DNA sensors were improved by replacing glass slide with PS substrates.The cDNA array sensors can bear 80℃of high temperature,75% of humidity,3.6 kLx of irradiation and keep stable within 10 days when they are exposed in air.Good performances of the K^+ISE and the cDNA array sensor are attributed to the large internal surface area and the easily modified microstructure of PS.