Effect of graphene nanoplatelets(GNPs)addition on mechanical properties of magnesium–10wt%Titanium(Mg–10Ti)alloy is investigated in current work.The Mg-(10Ti+0.18GNPs)composite was synthesized using the semi powder ...Effect of graphene nanoplatelets(GNPs)addition on mechanical properties of magnesium–10wt%Titanium(Mg–10Ti)alloy is investigated in current work.The Mg-(10Ti+0.18GNPs)composite was synthesized using the semi powder metallurgy method followed by hot extrusion.Microstructural characterization results revealed the uniform distribution of reinforcement(Ti+GNPs)particles in the matrix,therefore(Ti+GNPs)particles act as an effective reinforcing filler to prevent the deformation.Room temperature tensile results showed that the addition of Ti+GNPs to monolithic Mg lead to increase in 0.2%yield strength(0.2%YS),ultimate tensile strength(UTS),and failure strain.Scanning Electron Microscopy(SEM),Energy-Dispersive X-ray Spectroscopy(EDS)and X-Ray Diffraction(XRD)were used to investigate the surface morphology,elemental dispersion and phase analysis,respectively.展开更多
Magnesium-based biomaterials have recently gained great attention as promising candidates for the new generation of biodegradable implants.This study investigated the mechanical performance and biodegradation behaviou...Magnesium-based biomaterials have recently gained great attention as promising candidates for the new generation of biodegradable implants.This study investigated the mechanical performance and biodegradation behaviour of magnesium-zinc/hydroxyapatite(Mg-Zn/HA)composites fabricated by different powder mixing techniques.A single step mixing process involved mechanical alloying or mechanical milling techniques,while double step processing involved a combination of both mechanical alloying and mechanical milling.Optimum mechanical properties of the composite were observed when the powders were prepared using single step processing via mechanical alloying technique.However,Mg-Zn/HA composite fabricated through single step processing via mechanical milling technique was found to have the most desirable low degradation rate coupled with highest bioactivity.The composite achieved the lowest degradation rate of 0.039×10^−3 mm/year as measured by immersion test and 0.0230 mm/year as measured by electrochemical polarization.Ca:P ratio of the composite also slightly more than enough to aid the initial bone mineralization,that is 1:1.76,as the required Ca:P ratio for initial bone mineralization is between 1:1 and 1:1.67.展开更多
The effect of limestone powder and fly ash on magnesium sulfate resistance of mortar was studied by testing on the strength, expansion and hydration products of the specimens stored in MgSO4 solution at certain period...The effect of limestone powder and fly ash on magnesium sulfate resistance of mortar was studied by testing on the strength, expansion and hydration products of the specimens stored in MgSO4 solution at certain periods. The experimental results show that the strength of mortar stored in MgSO4 solution increases a little before 28 d, but decreases fast subsequently. The more the contents of limestone powder and fly ash, the less the strength losses. Mortar swells in the MgSO4 solution with the soaking time. And the more the contents of limestone powder and fly ash, the less the expansion rate is. The expansion or strength loss of mortars results from the expansion of gypsum, as well as the loss of Ca(OH)2 and other hydration products of cement. The magnesium sulfate resistance of the mortars containing limestone powder and fly ash is high.展开更多
A high-pressure laser ignition and combustion system with adjustable oxidizer gas atmosphere is established to investigate the ignition and combustion characteristics of boron-magnesium(BM)com-posite powders.An igniti...A high-pressure laser ignition and combustion system with adjustable oxidizer gas atmosphere is established to investigate the ignition and combustion characteristics of boron-magnesium(BM)com-posite powders.An ignition and combustion model of BM powders is established and validated in the present study.The results show that increasing water content,O_(2) content and Mg content all result in shorter ignition delay time of BM powders,among which the effect of water content is the most obvious.However,ignition delay time increases as pressure increases.The combustion time decreases with increasing Mg content and ambient pressure but increases with water content.With the increase of O_(2) content,combustion time of BM powders first increases and then decreases,which means a critical O_(2) content exists above which combustion time decreases.The results show that there exists a trade-off between ignition and combustion performance of BM composite powders.展开更多
Laser powder bed fusion(L-PBF)of Mg alloys has provided tremendous opportunities for customized production of aeronautical and medical parts.Layer thickness(LT)is of great significance to the L-PBF process but has not...Laser powder bed fusion(L-PBF)of Mg alloys has provided tremendous opportunities for customized production of aeronautical and medical parts.Layer thickness(LT)is of great significance to the L-PBF process but has not been studied for Mg alloys.In this study,WE43 Mg alloy bulk cubes,porous scaffolds,and thin walls with layer thicknesses of 10,20,30,and 40μm were fabricated.The required laser energy input increased with increasing layer thickness and was different for the bulk cubes and porous scaffolds.Porosity tended to occur at the connection joints in porous scaffolds for LT40 and could be eliminated by reducing the laser energy input.For thin wall parts,a large overhang angle or a small wall thickness resulted in porosity when a large layer thicknesses was used,and the porosity disappeared by reducing the layer thickness or laser energy input.A deeper keyhole penetration was found in all occasions with porosity,explaining the influence of layer thickness,geometrical structure,and laser energy input on the porosity.All the samples achieved a high fusion quality with a relative density of over 99.5%using the optimized laser energy input.The increased layer thickness resulted to more precipitation phases,finer grain sizes and decreased grain texture.With the similar high fusion quality,the tensile strength and elongation of bulk samples were significantly improved from 257 MPa and 1.41%with the 10μm layer to 287 MPa and 15.12%with the 40μm layer,in accordance with the microstructural change.The effect of layer thickness on the compressive properties of porous scaffolds was limited.However,the corrosion rate of bulk samples accelerated with increasing the layer thickness,mainly attributed to the increased number of precipitation phases.展开更多
基金The present work was supported by the National Natural Science Funds of China(No.50725413)the Ministry of Science and Technology of China(MOST)(No.2010DFR50010 and 2011FU125Z07)Chongqing Science and Technology Commission(CSTC2013jcyjC60001).
文摘Effect of graphene nanoplatelets(GNPs)addition on mechanical properties of magnesium–10wt%Titanium(Mg–10Ti)alloy is investigated in current work.The Mg-(10Ti+0.18GNPs)composite was synthesized using the semi powder metallurgy method followed by hot extrusion.Microstructural characterization results revealed the uniform distribution of reinforcement(Ti+GNPs)particles in the matrix,therefore(Ti+GNPs)particles act as an effective reinforcing filler to prevent the deformation.Room temperature tensile results showed that the addition of Ti+GNPs to monolithic Mg lead to increase in 0.2%yield strength(0.2%YS),ultimate tensile strength(UTS),and failure strain.Scanning Electron Microscopy(SEM),Energy-Dispersive X-ray Spectroscopy(EDS)and X-Ray Diffraction(XRD)were used to investigate the surface morphology,elemental dispersion and phase analysis,respectively.
基金The authors would like thank to Universiti Sains Malaysia for FRGS Grant No.203/PBAHAN/6071386 and financial scholarship from Ministry of Higher Education of Malaysia.
文摘Magnesium-based biomaterials have recently gained great attention as promising candidates for the new generation of biodegradable implants.This study investigated the mechanical performance and biodegradation behaviour of magnesium-zinc/hydroxyapatite(Mg-Zn/HA)composites fabricated by different powder mixing techniques.A single step mixing process involved mechanical alloying or mechanical milling techniques,while double step processing involved a combination of both mechanical alloying and mechanical milling.Optimum mechanical properties of the composite were observed when the powders were prepared using single step processing via mechanical alloying technique.However,Mg-Zn/HA composite fabricated through single step processing via mechanical milling technique was found to have the most desirable low degradation rate coupled with highest bioactivity.The composite achieved the lowest degradation rate of 0.039×10^−3 mm/year as measured by immersion test and 0.0230 mm/year as measured by electrochemical polarization.Ca:P ratio of the composite also slightly more than enough to aid the initial bone mineralization,that is 1:1.76,as the required Ca:P ratio for initial bone mineralization is between 1:1 and 1:1.67.
基金Funded by the Specialized Research Fund for the Doctoral Program of Higher Education of China (No.200804861060)
文摘The effect of limestone powder and fly ash on magnesium sulfate resistance of mortar was studied by testing on the strength, expansion and hydration products of the specimens stored in MgSO4 solution at certain periods. The experimental results show that the strength of mortar stored in MgSO4 solution increases a little before 28 d, but decreases fast subsequently. The more the contents of limestone powder and fly ash, the less the strength losses. Mortar swells in the MgSO4 solution with the soaking time. And the more the contents of limestone powder and fly ash, the less the expansion rate is. The expansion or strength loss of mortars results from the expansion of gypsum, as well as the loss of Ca(OH)2 and other hydration products of cement. The magnesium sulfate resistance of the mortars containing limestone powder and fly ash is high.
基金the supports from National Natural Science Foundation of China(grant Nos.52276087,51806048,51776175)the Fundamental Research Funds for the Central Universities(grant No.D5000210602)+2 种基金the Key Fundamental Strengthening Project(grant Nos.2019-JCJQ-ZD-083-05,2021-JCJQ-J-0401)the Foundation of Key Laboratory(grant No.6142701190106),Natural Science Foundation of Jiangsu Province(grant No.BK20210854)Natural Science Foundation of Jiangsu Universities(grant No.20KJB470009).
文摘A high-pressure laser ignition and combustion system with adjustable oxidizer gas atmosphere is established to investigate the ignition and combustion characteristics of boron-magnesium(BM)com-posite powders.An ignition and combustion model of BM powders is established and validated in the present study.The results show that increasing water content,O_(2) content and Mg content all result in shorter ignition delay time of BM powders,among which the effect of water content is the most obvious.However,ignition delay time increases as pressure increases.The combustion time decreases with increasing Mg content and ambient pressure but increases with water content.With the increase of O_(2) content,combustion time of BM powders first increases and then decreases,which means a critical O_(2) content exists above which combustion time decreases.The results show that there exists a trade-off between ignition and combustion performance of BM composite powders.
基金funded by the National Key Research and Development Program of China(2018YFE0104200)National Natural Science Foundation of China(51875310,52175274,82172065)Tsinghua Precision Medicine Foundation.
文摘Laser powder bed fusion(L-PBF)of Mg alloys has provided tremendous opportunities for customized production of aeronautical and medical parts.Layer thickness(LT)is of great significance to the L-PBF process but has not been studied for Mg alloys.In this study,WE43 Mg alloy bulk cubes,porous scaffolds,and thin walls with layer thicknesses of 10,20,30,and 40μm were fabricated.The required laser energy input increased with increasing layer thickness and was different for the bulk cubes and porous scaffolds.Porosity tended to occur at the connection joints in porous scaffolds for LT40 and could be eliminated by reducing the laser energy input.For thin wall parts,a large overhang angle or a small wall thickness resulted in porosity when a large layer thicknesses was used,and the porosity disappeared by reducing the layer thickness or laser energy input.A deeper keyhole penetration was found in all occasions with porosity,explaining the influence of layer thickness,geometrical structure,and laser energy input on the porosity.All the samples achieved a high fusion quality with a relative density of over 99.5%using the optimized laser energy input.The increased layer thickness resulted to more precipitation phases,finer grain sizes and decreased grain texture.With the similar high fusion quality,the tensile strength and elongation of bulk samples were significantly improved from 257 MPa and 1.41%with the 10μm layer to 287 MPa and 15.12%with the 40μm layer,in accordance with the microstructural change.The effect of layer thickness on the compressive properties of porous scaffolds was limited.However,the corrosion rate of bulk samples accelerated with increasing the layer thickness,mainly attributed to the increased number of precipitation phases.