铝合金CO_(2)激光-TIG电弧复合焊接试验研究 被引量:13
1
作者 雷正龙 陈彦宾 +4 位作者 李颖 孙忠绍 陈济轮 董鹏 赵婷 《航天制造技术》 2012年第4期35-37,共3页
以LF6铝合金为材料,开展了CO2激光-TIG电弧复合焊接工艺试验研究。试验结果表明,与单激光或TIG电弧比较,激光-TIG复合焊接可以提高焊缝熔深,改善焊缝成形,降低气孔和下塌等焊接缺陷。在此基础上,进一步研究了不同工艺参数对焊缝成形的影... 以LF6铝合金为材料,开展了CO2激光-TIG电弧复合焊接工艺试验研究。试验结果表明,与单激光或TIG电弧比较,激光-TIG复合焊接可以提高焊缝熔深,改善焊缝成形,降低气孔和下塌等焊接缺陷。在此基础上,进一步研究了不同工艺参数对焊缝成形的影响,探索了铝合金激光-TIG电弧复合焊接的可行性。 展开更多
关键词 激光?tig 电弧复合 焊缝成形 工艺参数 铝合金
下载PDF
建筑钢/铝的激光-电弧焊铆与组织性能 被引量:1
2
作者 徐亮亮 王克勤 许达哲 《应用激光》 CSCD 北大核心 2022年第10期9-17,共9页
采用激光-TIG电弧复合热源对建筑用Q460钢/6061铝合金进行了焊铆复合连接,研究了直流TIG电流对铝/钢焊铆复合接头成形、接头形貌和力学性能的影响。结果表明,直流TIG电流为75~115 A时,钢/铝焊铆复合接头试样都成形良好,焊点及周围区域... 采用激光-TIG电弧复合热源对建筑用Q460钢/6061铝合金进行了焊铆复合连接,研究了直流TIG电流对铝/钢焊铆复合接头成形、接头形貌和力学性能的影响。结果表明,直流TIG电流为75~115 A时,钢/铝焊铆复合接头试样都成形良好,焊点及周围区域未见异常裂纹、气孔等焊接缺陷;随着直流TIG电流从75 A增加至115 A,焊点未熔区域面积逐渐减小、铝板焊接熔深逐渐长大,钢/铝焊铆复合接头的拉剪载荷先增大后减小,在直流TIG电流为95 A时取得最大值;直流TIG电流为75 A时,钢/铝焊铆复合接头呈纽扣断裂形态,其余接头呈拉拔断裂形态;适宜的直流TIG电流为95 A,此时焊点成形良好,焊接熔深为350 mm,拉剪载荷为5.52 kN。 展开更多
关键词 Q460钢/6061铝合金 激光-tig电弧复合焊 形貌 力学性能
原文传递
Novel hybrid method: pulse CO_2 laser-TIG hybrid welding by coordinated control 被引量:1
3
作者 陈彦宾 雷正龙 +2 位作者 李俐群 吴林 解成 《China Welding》 EI CAS 2006年第1期20-25,共6页
In continuous wave CO2 laser-TlG hybrid welding process, the laser energy is not fully utilized because of the absorption and defocusing by plasma in the arc space. Therefore, the optimal welding result can only be ac... In continuous wave CO2 laser-TlG hybrid welding process, the laser energy is not fully utilized because of the absorption and defocusing by plasma in the arc space. Therefore, the optimal welding result can only be achieved in a limited energy range. In order to improve the welding performance further, a novel hybrid welding method--pulse CO2 laser-TIG arc hybrid welding by coordinated control is proposed and investigated. The experimental results indicate that, compared with continuous wave CO2 laser-TIG hybrid welding, the absorption and defocusing of laser energy by plasma are decreased further, and at the same time, the availability ratio of laser and arc energy can be increased when a coordinated frequency is controlled. As a result, the weld appearance is also improved as well as the weld depth is deepened. Furthermore, the effect of frequency and phase of pulse laser and TIG arc on the arc images and welding characteristics is also studied. However, the novel hybrid method has great potentials in the application of industrials from views of techniques and economy. 展开更多
关键词 CO2 laser-tig hybrid welding pulse coordinated control welding characteristics arc images