期刊文献+
共找到2篇文章
< 1 >
每页显示 20 50 100
放氢温度对吸氢后La_(1-x)Ce_xFe_(11.44)Si_(1.56)合金磁热性能的影响 被引量:2
1
作者 夏伟 黄焦宏 +3 位作者 刘翠兰 松林 张文佳 特古斯 《稀土》 EI CAS CSCD 北大核心 2016年第3期50-55,共6页
利用X射线衍射仪(XRD)和VSM测量La_(1-x)Ce_xFe_(11.44)Si_(1.56)合金吸氢前后的相结构及磁性曲线,利用DSC测量了La_(0.8)Ce_(0.2)Fe_(11.44)Si_(1.56)Hy的热重曲线。结果表明,La_(1-x)Ce_xFe_(11.44)Si_(1.56)合金及其氢化物的主相均为... 利用X射线衍射仪(XRD)和VSM测量La_(1-x)Ce_xFe_(11.44)Si_(1.56)合金吸氢前后的相结构及磁性曲线,利用DSC测量了La_(0.8)Ce_(0.2)Fe_(11.44)Si_(1.56)Hy的热重曲线。结果表明,La_(1-x)Ce_xFe_(11.44)Si_(1.56)合金及其氢化物的主相均为NaZn_(13)型立方结构,吸氢后合金的居里温度明显升高,在室温空气中放置一段时间后,仍能保持良好的稳定性;La_(0.8)Ce_(0.2)Fe_(11.44)Si_(1.56)Hy合金约从483 K到708 K一直处于失重状态,氢化物的失重率为0.19%;通过提高放氢温度,La_(0.9)Ce_(0.1)Fe_(11.44)Si_(1.56)Hy合金的居里温度降低,放氢温度每提高10 K居里温度下降10 K左右,但对合金的等温磁熵变影响很小,熵变最小的样品与无放氢样品的熵变相差仅0.616 J/(kg·K)。 展开更多
关键词 放氢温度 居里温度 等温磁熵变 la1-xcexfe11.44si1.56hy
原文传递
Influence of partial substitution of cerium for lanthanum on magnetocaloric properties of La_(1–x)Ce_xFe_(11.44)Si_(1.56) and their hydrides 被引量:2
2
作者 慕利娟 黄焦宏 +3 位作者 张文佳 刘翠兰 王高峰 赵增祺 《Journal of Rare Earths》 SCIE EI CAS CSCD 2014年第12期1135-1139,共5页
The structure and magnetocaloric properties of La1–xCexFe11.44Si1.56 and their hydrides La1–xCexFe11.44Si1.56Hy(x=0, 0.1, 0.2, 0.3, 0.4) were investigated.The samples crystallized mainly in the cubic Na Zn13-type ... The structure and magnetocaloric properties of La1–xCexFe11.44Si1.56 and their hydrides La1–xCexFe11.44Si1.56Hy(x=0, 0.1, 0.2, 0.3, 0.4) were investigated.The samples crystallized mainly in the cubic Na Zn13-type structure with a small amount of α-Fe phase as impurity.The lattice constants and Curie temperature presented the same change tendency with increasing of Ce content.For the hydrides, the influence of Ce content on lattice constants was weakened and the values of H concentration y were approximate to be 1.56.The La1–xCexFe11.44Si1.56 compounds exhibited large values of isothermal entropy change –ΔSm around the Curie temperature TC under a low magnetic field change of 1.5 T.The value of –ΔSm increased and then decreased with increasing Ce content, reached the maximum, 26.07 J/kg·K for x=0.3.TC increased up to the vicinity of room temperature by hydrogen absorption for the Ce substituted compounds, but TC only slightly decreased with increasing Ce content.The first-order metamagnetic transition was still kept in the hydrides and the maximum values of –ΔSm were lower than those of the La1–xCexFe11.44Si1.56 compounds, but still remained large values, about 10.5 J/kg K under a magnetic field change of 1.5 T.The values of –ΔSm were nearly independent of the Ce content and did not increase with increasing x for the hydrides.The La1–xCexFe11.44Si1.56Hy(x=0–0.4) hydrides exhibited large magnetic entropy changes, small hysteresis loss and effective refrigerant capacity covered the room temperature range from 305 to 317 K.These hydrides are very useful for the magnetic refrigeration applications near room temperature under low magnetic field change. 展开更多
关键词 la1xcexfe11.44si1.56hy isothermal entropy change Curie temperature magnetic hysteresis loss rare earths
原文传递
上一页 1 下一页 到第