Influence of La precursors on structure and properties of CeO_2-ZrO_2-Al_2O_3 composite oxides 被引量:1
1
作者 You-feng LI Yue-hui HE +1 位作者 Guo-qing LIU Ling-wei ZENG 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2018年第4期739-747,共9页
Three La-doped CeO2-ZrO2-Al2O3(CZA)composite oxide samples,namely,CZA-I,CZA-II and CZA-III,were prepared following a co-precipitation method in the presence of La2O3,La(NO3)3-6H2O and H[La(EDTA)]-16H2O precursors,resp... Three La-doped CeO2-ZrO2-Al2O3(CZA)composite oxide samples,namely,CZA-I,CZA-II and CZA-III,were prepared following a co-precipitation method in the presence of La2O3,La(NO3)3-6H2O and H[La(EDTA)]-16H2O precursors,respectively.When the precursor samples are sintered at 1000°C,the as-prepared composite oxides mainly exhibit the CeO2-ZrO2 cubic fluorite phase,while theγ-Al2O3 andδ-Al2O3 phases appear when the precursor samples are subjected to sintering at 1100 and 1200°C.CZA-III exhibits improved redox properties after high-temperature treatment compared with CZA-I and CZA-II.CZA-III presents the largest surface area of 97.46 m2/g among the three CZAs when the CZA-III precursor sample is sintered at 1000°C.Furthermore,the corresponding oxygen storage capacity(OSC)is the largest with value of 400.27μmol/g when CZA-III precursor sample is sintered at 1000°C.Additionally,CZA-III exhibits the best thermal stability and the highest reduction temperature.However,by increasing the sintering temperature to 1200°C,there is a dramatic decline in the properties of surface area and OSC.And a decrease for CZA-III in surface area by 58.94%and a decrease of the OSC value by 74.56%are observed. 展开更多
关键词 la precursor ceria-zirconia solid solution composite oxide texture structure redox property
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部