Diffusion couples,WC/Co-1at.%C,V8C7/Co,and WC/Co-0.3wt.%V8C7 were constructed and annealed at temperatures ranging from 1100 to 1300℃. The concentration profile of V and W atoms in these couples were measured by EPMA...Diffusion couples,WC/Co-1at.%C,V8C7/Co,and WC/Co-0.3wt.%V8C7 were constructed and annealed at temperatures ranging from 1100 to 1300℃. The concentration profile of V and W atoms in these couples were measured by EPMA. Aided by Thermo-calc & DICTRA software package,the concentration profiles of W and V in established diffusion couples were calculated by the moving boundary model according to revised dynamic parameters and MOB database,respectively. Then the concentration profile of W in Co binder during sintering WC-Co cemented carbide was simulated by the Cell model. It can provide reference for composition and sintering process design of cemented carbides with high performance. Meanwhile,the validity of revised dynamic parameters of the W-C-Co-V system is verified by the comparison of experimental and simulated results.展开更多
AISI H13 hot work tool steel is widely used for hot forging, hot-extrusion and die-casting because of its high temperature strength, impact toughness, heat checking resistance and wear resistance, etc. The thermally i...AISI H13 hot work tool steel is widely used for hot forging, hot-extrusion and die-casting because of its high temperature strength, impact toughness, heat checking resistance and wear resistance, etc. The thermally induced surface damage, i. e., thermal fatigne,is believed to be controlled by the magnitude of the imposed cyclic strain. The thermal fatigue on the surface of hot working die, which is responsible to the initiation of the cracks, is reported to result in more than 80 % of the failure of dies.展开更多
文摘建立了热等静压扩散连接的数学模型,利用DICTRA软件与Thermal-Calc软件相结合的方法计算了不同温度、不同时间热等静压扩散连接界面反应层元素的互扩散规律与相分布情况,并根据计算结果给出了建议的扩散连接工艺范围,为工艺参数的设计提供了理论依据.计算结果表明:与时间相比,温度对扩散连接界面的元素扩散影响更大.针对DD407/FGH95合金系,扩散连接温度应选择在1120—1210℃的温度区间内.综合考虑扩散连接的元素互扩散区宽度及界面元素富集情况,1120℃时扩散连接的合理扩散时间为3—5 h,1170和1210℃时扩散连接的合理扩散时间为1—3 h.
基金the National Natural Science Foundation of China (No. 50471101)the Flan-ders-China Bilateral Project BIL 02/04.
文摘Diffusion couples,WC/Co-1at.%C,V8C7/Co,and WC/Co-0.3wt.%V8C7 were constructed and annealed at temperatures ranging from 1100 to 1300℃. The concentration profile of V and W atoms in these couples were measured by EPMA. Aided by Thermo-calc & DICTRA software package,the concentration profiles of W and V in established diffusion couples were calculated by the moving boundary model according to revised dynamic parameters and MOB database,respectively. Then the concentration profile of W in Co binder during sintering WC-Co cemented carbide was simulated by the Cell model. It can provide reference for composition and sintering process design of cemented carbides with high performance. Meanwhile,the validity of revised dynamic parameters of the W-C-Co-V system is verified by the comparison of experimental and simulated results.
文摘AISI H13 hot work tool steel is widely used for hot forging, hot-extrusion and die-casting because of its high temperature strength, impact toughness, heat checking resistance and wear resistance, etc. The thermally induced surface damage, i. e., thermal fatigne,is believed to be controlled by the magnitude of the imposed cyclic strain. The thermal fatigue on the surface of hot working die, which is responsible to the initiation of the cracks, is reported to result in more than 80 % of the failure of dies.