In this investigation, an attempt has been made to develop Al6061-Frit particulate metal matrix composites through stir casting technique using metal molds and to study the corrosion behaviour. Pre heated frit particl...In this investigation, an attempt has been made to develop Al6061-Frit particulate metal matrix composites through stir casting technique using metal molds and to study the corrosion behaviour. Pre heated frit particles were added to matrix as reinforcement. Al6061 containing 2 wt% to 8 wt % in steps of 2 wt % of frit particulate composites were prepared. Corrosion tests were conducted by using Potentiostat model SEP238C where 3.5% NaCl solution was used as corrodent. The corrosion rate of metal matrix composites was lower than that of matrix material Al6061 under the corrosive atmosphere for both un-heat treated and heat treated conditions.展开更多
文摘In this investigation, an attempt has been made to develop Al6061-Frit particulate metal matrix composites through stir casting technique using metal molds and to study the corrosion behaviour. Pre heated frit particles were added to matrix as reinforcement. Al6061 containing 2 wt% to 8 wt % in steps of 2 wt % of frit particulate composites were prepared. Corrosion tests were conducted by using Potentiostat model SEP238C where 3.5% NaCl solution was used as corrodent. The corrosion rate of metal matrix composites was lower than that of matrix material Al6061 under the corrosive atmosphere for both un-heat treated and heat treated conditions.