期刊文献+
共找到3篇文章
< 1 >
每页显示 20 50 100
Synthesis and Properties of Novel Polyimide Fibers Containing Phosphorus Groups in the Side Chain (DATPPO) 被引量:1
1
作者 Yong Zhao Guo-min Li +3 位作者 Fang-fang Liu Xue-min Dai 董志鑫 邱雪鹏 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2017年第3期372-385,共14页
A series of polyamic acid copolymers(co-PAAs) containing phosphorous groups in the side chains were synthesized from [2,5-bis(4-aminophenoxy) phenyl] diphenylphosphine oxide(DATPPO) and 4,4′-oxydianiline(ODA) with 3,... A series of polyamic acid copolymers(co-PAAs) containing phosphorous groups in the side chains were synthesized from [2,5-bis(4-aminophenoxy) phenyl] diphenylphosphine oxide(DATPPO) and 4,4′-oxydianiline(ODA) with 3,3′,4,4′-biphenyltetracarboxylic dianhydride(s-BPDA) through the polycondensation in N,N′-dimethyacetamide(DMAc). The co-PAA solutions were spun into fibers by a dry-jet wet spinning process followed by thermal imidization to obtain co-polyimide(co-PI) fibers. FTIR spectra and elemental analysis confirmed the chemical structure of PI fibers. SEM results indicated that the resulting PI fibers had a smooth and dense surface, a uniform and circle-shape diameter. The thermogravimetric measurements showed that with the increase of DATPPO content, the resulting PI fibers possessed high decomposition temperature and residual char yield, indicating that the PI fibers had good thermal stability. The corresponding limiting oxygen index(LOI) values from the experiment results showed that the co-PI fibers possessed good flame-retardant property. Furthermore, the mechanical properties of the co-PI fibers were investigated systematically. When the DATPPO content increased, the tensile strength and initial modulus of the co-PI fibers decreased. However, the mechanical properties were improved by increasing the draw ratio of the fibers. When the draw ratio was up to 2.5, the tensile strength and initial modulus of the co-PI fibers reached up to 0.64 and 10.02 GPa, respectively. The WAXD results showed that the order degree of amorphous matter increased with increased stretching. In addition, the SAXS results displayed that valuably drawing the fibers could eliminate the voids inside and lead to better mechanical property. WAXD revealed that the orientation of the amorphous polymer influenced the mechanical properties of the fibers. 展开更多
关键词 [2 5-bis(4-aminophenoxy) phenyl] diphenylphosphine oxide Dry-jet wet spinning process Phosphorous Polyimide fibers
原文传递
含活性基聚酰亚胺薄膜的研制 被引量:4
2
作者 李恩 虞鑫海 +2 位作者 樊良子 徐永芬 刘万章 《绝缘材料》 CAS 北大核心 2011年第6期12-15,共4页
将3,5-双(4-氨基苯氧基)苯甲酸(35BAPBA)、二苯醚四羧酸二酐(ODPA)进行缩聚反应,得到聚酰胺酸(PAA)溶液,然后经过合适的固化工艺使其脱水热亚胺化,制得含羧基的聚酰亚胺薄膜,并对其性能进行研究。结果表明:含羧基的聚酰亚胺薄膜具有良... 将3,5-双(4-氨基苯氧基)苯甲酸(35BAPBA)、二苯醚四羧酸二酐(ODPA)进行缩聚反应,得到聚酰胺酸(PAA)溶液,然后经过合适的固化工艺使其脱水热亚胺化,制得含羧基的聚酰亚胺薄膜,并对其性能进行研究。结果表明:含羧基的聚酰亚胺薄膜具有良好的紫外吸收性能、疏水性、电绝缘性等。 展开更多
关键词 3 5-双(4-氨基苯氧基)苯甲酸 聚酰胺酸 聚酰亚胺薄膜 性能研究
下载PDF
3,5-双(4-氨基苯氧基)苯甲酸的合成及其聚酰亚胺薄膜的性能研究 被引量:1
3
作者 李恩 虞鑫海 +1 位作者 徐永芬 刘万章 《化学与粘合》 CAS 2012年第3期18-22,共5页
合成3,5-双(4-氨基苯氧基)苯甲酸(35BAPBA)。其方法为3,5-二羟基苯甲酸(35DHBA)和对氯硝基苯(PCNB)通过缩合反应,合成得到了3,5-双(4-硝基苯氧基)苯甲酸(35BNPBA);然后,进一步还原,得到3,5-T2(4-氨基苯氧基)苯甲酸(3... 合成3,5-双(4-氨基苯氧基)苯甲酸(35BAPBA)。其方法为3,5-二羟基苯甲酸(35DHBA)和对氯硝基苯(PCNB)通过缩合反应,合成得到了3,5-双(4-硝基苯氧基)苯甲酸(35BNPBA);然后,进一步还原,得到3,5-T2(4-氨基苯氧基)苯甲酸(35BAPBA),基于35BAPBA单体,制得多种结构的含羧基芳香族聚酰亚胺薄膜,并对这些薄膜的性能进行研究。制得的3,5-双(4-氨基苯氧基)苯甲酸(35BAPBA)的熔点为245.8℃,且纯度高。各类薄膜的透过率均可达80%以上,具有良好的紫外吸收性能;吸水性均小于3%,具有优异的疏水性能;其拉伸强度在15~56MPa之间。 展开更多
关键词 3 5-双(4-氨基苯氧基)苯甲酸(35BAPBA) 含羧基聚酰亚胺 合成 性能研究
原文传递