Corrosion mechanism of H_2O on Sm_2Fe_(17) and nitrogenation process of corroded Sm_2Fe_(17) 被引量:2
1
作者 Jianwei Xu Jingwu Zheng +7 位作者 Haibo Chen Liang Qiao Yao Ying Wei Cai Wangchang Li Jing Yu Min Lin Shenglei Che 《Journal of Rare Earths》 SCIE EI CAS CSCD 2019年第6期638-644,共7页
Sm_2 Fe_(17) prepared by reduction-diffusion method needs to be washed with water to remove calcium oxide. Electrochemical corrosion occurs when Sm_2 Fe_(17) powder is in contact with liquid water. Corrosion mechanism... Sm_2 Fe_(17) prepared by reduction-diffusion method needs to be washed with water to remove calcium oxide. Electrochemical corrosion occurs when Sm_2 Fe_(17) powder is in contact with liquid water. Corrosion mechanism of H_2 O on Sm_2 Fe_(17) powder and nitrogenation process of corroded Sm_2 Fe_(17) were studied by analyzing the structure and morphology. It is indicated that the metallic hydroxide forms and deposits on the Sm_2 Fe_(17) powder surfaces during water corrosion. At the same time, oxygen and hydrogen enter the unit cell of Sm2 Fe_(17), causing a slight increase in Curie temperature. In the subsequent nitriding process,the hydroxide is dehydrated and hydrogen is desorbed. The resulting oxide reacts with Sm_2 Fe_(17)N_x to form a-Fe and Sm_2 O_3. Thermodynamic calculations using the HSC Chemistry 6.0 software indicate that the reaction can occur spontaneously. The effect of water corrosion on the magnetic properties of the nitride can be eliminated by hydrogen reduction prior to nitriding. 展开更多
关键词 Sm2fe17 NITROGENATION Reduction-diffusion method Water CORROSION α-fe formation RARE earths
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部