Formation of hierarchical Fe7Se8 nanorod bundles with enhanced sodium storage properties 被引量:3
1
作者 Wenzhi Tian Wenzhe Ma +3 位作者 Zhenyu Feng Fang Tian Haibo Li Jing Liu 《Journal of Energy Chemistry》 SCIE EI CAS CSCD 2020年第5期97-105,共9页
Ordered hierarchical architectures are attractive candidates for electrochemical energy storage applications.Herein,a facile self-template strategy is applied to prepare Fe7Se8 architectures with a monolithic structur... Ordered hierarchical architectures are attractive candidates for electrochemical energy storage applications.Herein,a facile self-template strategy is applied to prepare Fe7Se8 architectures with a monolithic structure via a self-synthesized single precursor and subsequent calcination at high temperature.With the support of oleylamine,the precursor is structurally targeted to engineer the Fe7Se8 microstructure,featuring nanorod bundles arranged along the longitudinal direction.Because of their ordered hierarchical structure,the Fe7Se8 nanorod bundles deliver a high reversible capacity of 300 m Ah g^-1 at 0.5 A g^-1,along with exceptional rate capability up to 20 A g^-1 and long-term cycle life over 8000 cycles,which represents the highest stability of Fe7Se8 anodes for sodium-ion batteries reported to date.The feasibility of the present strategy to prepare metal selenide structures highlights its promising potential for the rational and effective engineering of electrode materials responsible for the electrochemical performance of energy storage systems. 展开更多
关键词 Fe7Se8 HIERARCHICAL structure nanorod bundles Sodium-ion BATTERIES OLEYLAMINE
下载PDF
不同形貌氧化锌的简易合成及其光催化降解环丙沙星废水 被引量:5
2
作者 张宪 石凤琼 张格红 《北京化工大学学报(自然科学版)》 CAS CSCD 北大核心 2016年第3期80-84,共5页
以硝酸锌、水合肼、氢氧化钠、氯化钾为原料,通过简单的水热法,在100℃下反应2 h制备出形貌均一、分散性好的氧化锌纳米棒、纳米棒束和纳米花。利用XRD、SEM、UV-vis对所制备样品的组成和形貌进行表征。以紫外灯为光源,环丙沙星为降解对... 以硝酸锌、水合肼、氢氧化钠、氯化钾为原料,通过简单的水热法,在100℃下反应2 h制备出形貌均一、分散性好的氧化锌纳米棒、纳米棒束和纳米花。利用XRD、SEM、UV-vis对所制备样品的组成和形貌进行表征。以紫外灯为光源,环丙沙星为降解对象,考察不同形貌的氧化锌对降解抗生素废水的活性。实验结果表明:适量Na OH的加入有利于纳米花的形成,KCl的加入则促使纳米棒束结构的形成;纳米棒、纳米棒束及纳米花ZnO的固体紫外-可见光谱显示其吸收边缘依次出现一定的红移;在汞灯光照下反应120 min后,ZnO纳米棒、纳米棒束及纳米花对环丙沙星的降解率分别为45.5%、60.3%和90.2%。 展开更多
关键词 光催化 氧化锌 纳米棒 纳米棒束 纳米花 环丙沙星
原文传递