The effects of lance height and bottom blown flowrate on the mixed time, the splashing amount, the penetrating depth, and the level fluctuation of an 85 t combined blown converter have been studied using a water model...The effects of lance height and bottom blown flowrate on the mixed time, the splashing amount, the penetrating depth, and the level fluctuation of an 85 t combined blown converter have been studied using a water model. The results show that the maximal stirring energy is provided to the bath at the top lance height of about 50-100 mm. When the top lance height is in the range ofg0- 110 mm, the splashing amount caused by the top jet can reach the maximal value. The appropriate operational parameters of Chongqing Iron and Steel Company (CISC) converter have been established that the top lance height is 1600-1760 mm and the bottom blowing flowrate is 240-480 Nm^3/h in the primary phase of a heat, 1100-1300 mm and 160-200 Nm^3/h in the second phase, and 1040-1120 mm and 200-350 Nm^3/h in the end phase. Also, the trial shows that the metallurgical result of the studied blow pattern is better than that of the former pattern. At the starting 3-4 min of a heat, the strong splashing is eliminated. 2008 University of Science and Technology Beijing. All rights reserved.展开更多
A new method was presented to constrain deformation and oscillations of liquid metal free surface by using a high frequency magnetic field. A magnetic field generator was designed to investigate its feasibility using ...A new method was presented to constrain deformation and oscillations of liquid metal free surface by using a high frequency magnetic field. A magnetic field generator was designed to investigate its feasibility using numerical simulation and physical simulation. The results indicate the feasibility of controlling bulge deformation of liquid metal surface using magnetic pressure. Sunken deformation with a slight fluctuation occurs on the surface when magnetic pressure acts on the static liquid metal surface. The largest amplitude remains within i0.8 mm even if current rea- ches 1400 A. In case of the bump-type deformation, the magnetic pressure strengthens gravity field by the superpo- sition effect, dissipates the kinetic energy of metal flow impacting on free surface in advance, reduces the velocity of free surface, and decreases the bulge height. On the region without magnetic field, the liquid metal surface rises and tends to be flat because of the significant damping effect on surface fluctuation. The constraint strength of the mag- netic pressure increases with the augment of current intensity. However, different heights of bulge deformation should have a corresponding reasonable coil current for achieving the best constraint effect.展开更多
文摘The effects of lance height and bottom blown flowrate on the mixed time, the splashing amount, the penetrating depth, and the level fluctuation of an 85 t combined blown converter have been studied using a water model. The results show that the maximal stirring energy is provided to the bath at the top lance height of about 50-100 mm. When the top lance height is in the range ofg0- 110 mm, the splashing amount caused by the top jet can reach the maximal value. The appropriate operational parameters of Chongqing Iron and Steel Company (CISC) converter have been established that the top lance height is 1600-1760 mm and the bottom blowing flowrate is 240-480 Nm^3/h in the primary phase of a heat, 1100-1300 mm and 160-200 Nm^3/h in the second phase, and 1040-1120 mm and 200-350 Nm^3/h in the end phase. Also, the trial shows that the metallurgical result of the studied blow pattern is better than that of the former pattern. At the starting 3-4 min of a heat, the strong splashing is eliminated. 2008 University of Science and Technology Beijing. All rights reserved.
基金Item Sponsored by National Natural Science Foundation of China(51474065,51574083)Doctoral Scientific Research Foundation of Liaoning Province of China(20141008)+1 种基金Fundamental Research Funds for Central Universities of China(L1509003)Program of Introducing Talents of Discipline to Universities of China(B07015)
文摘A new method was presented to constrain deformation and oscillations of liquid metal free surface by using a high frequency magnetic field. A magnetic field generator was designed to investigate its feasibility using numerical simulation and physical simulation. The results indicate the feasibility of controlling bulge deformation of liquid metal surface using magnetic pressure. Sunken deformation with a slight fluctuation occurs on the surface when magnetic pressure acts on the static liquid metal surface. The largest amplitude remains within i0.8 mm even if current rea- ches 1400 A. In case of the bump-type deformation, the magnetic pressure strengthens gravity field by the superpo- sition effect, dissipates the kinetic energy of metal flow impacting on free surface in advance, reduces the velocity of free surface, and decreases the bulge height. On the region without magnetic field, the liquid metal surface rises and tends to be flat because of the significant damping effect on surface fluctuation. The constraint strength of the mag- netic pressure increases with the augment of current intensity. However, different heights of bulge deformation should have a corresponding reasonable coil current for achieving the best constraint effect.