期刊文献+
共找到9篇文章
< 1 >
每页显示 20 50 100
先进高强度钢氢脆的研究进展 被引量:20
1
作者 罗洁 郭正洪 戎咏华 《机械工程材料》 CAS CSCD 北大核心 2015年第8期1-9,共9页
综述了先进高强度钢氢脆的研究进展,重点介绍了双相钢、相变诱发塑性钢、孪生诱发塑性钢、淬火-配分钢等材料中的氢脆特征、断裂模式、断口形貌特点以及相关的断裂机制,为揭示先进高强度钢的氢脆机理及提出相应的预防措施提供参考。
关键词 氢脆 双相钢 相变诱发塑性钢 孪生诱发塑性钢 淬火-配分钢
下载PDF
Effect of Heat Treatment on Microstructures and Mechanical Properties of Hot-Dip Galvanized DP Steels 被引量:8
2
作者 Enbao Pan Hongshuang Di +1 位作者 Guangwei Jiang Chengren Bao 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2014年第3期469-475,共7页
In order to simulate the hot-dipped galvanizing of dual-phase (DP) steel (wt%) 0.15C-0.1Si-1.7Mn, the DP steels were obtained by different annealing schedules. The effects of soaking temperature, time, and cooling... In order to simulate the hot-dipped galvanizing of dual-phase (DP) steel (wt%) 0.15C-0.1Si-1.7Mn, the DP steels were obtained by different annealing schedules. The effects of soaking temperature, time, and cooling rate on ferrite grain, volume fraction of martensite, and the fine structure of martensite were studied. Results showed that the yield strength (YS) of DP steel is sensitive to annealing schedule, while total elongation has no noticeable dependence on annealing schedule. Increasing soaking temperature from 790 to 850 ℃, the YS is the lowest at soaking temperature of 850 ℃. Changing CR1 from 6 to 24 ℃/s, the YS is the highest when CR1 is 12 ℃/s. Increasing soaking time from 30 to 100 s, the YS is the lowest at soaking time of 100 s. Besides, it was found that sufficient movable dislocations within ferrite grains and high martensite volume fraction can eliminate yield point elongation, decrease the YS, and increase ultimate tensile strength. Through TEM observations, it was also found that increasing annealing temperature promotes austenite transformation into twin martensite, and increases volume fraction of martensite at sufficient cooling rate. With increasing the martensite volume fraction, the deformation substructure in the ferrite is well developed. 展开更多
关键词 Advanced high strength steels (AHSS) dual-phase dp steel Microstructure Annealing temperature
原文传递
退火温度对DP980冷轧双相钢组织和力学性能的影响 被引量:3
3
作者 邢振环 张涛 +1 位作者 郭志凯 刘丽萍 《热加工工艺》 北大核心 2019年第12期172-174,共3页
以冷轧双相钢DP980为研究对象,探讨了退火温度对钢板组织性能的影响。结果表明:当退火温度从600℃增加到660℃,随着再结晶程度的逐步提高,强度逐渐降低;再结晶完成后,DP980钢退火温度从720℃增加到820℃,随着加热过程中获得的奥氏体含... 以冷轧双相钢DP980为研究对象,探讨了退火温度对钢板组织性能的影响。结果表明:当退火温度从600℃增加到660℃,随着再结晶程度的逐步提高,强度逐渐降低;再结晶完成后,DP980钢退火温度从720℃增加到820℃,随着加热过程中获得的奥氏体含量的增多,冷却后硬相的量更多,宏观表现为强度逐渐升高;由热处理过程的膨胀曲线结合组织观察发现,冷却后的硬相中既有马氏体又有贝氏体。 展开更多
关键词 退火温度 双相钢 再结晶 相变
下载PDF
双向钢的活动筋过拉伸工艺及模具设计 被引量:1
4
作者 张懃 《模具制造》 2013年第11期23-26,共4页
对于高等级的双相钢成形,克服扭曲回弹是个难以逾越的关隘。本文介绍了一种带活动拉伸筋的过拉伸模,用于成形DP钢内板件,取得了较好的效果。它为突破超高强度钢的工艺瓶颈提供了重要参考。
关键词 双相钢 扭曲回弹 活动拉伸筋 过拉伸
下载PDF
Experimental and numerical investigation of failure mode in geometrically imperfect DP590 steel
5
作者 ZHUANG XinCun XU Cheng ZHAO Zhen 《Science China(Technological Sciences)》 SCIE EI CAS CSCD 2015年第3期476-484,共9页
Various microstructure-level finite element models were generated according to the real microstructure of DP590 steel to capture the mechanical behavior and fracture mode.The failure mode of the dual-phase(DP)steels,m... Various microstructure-level finite element models were generated according to the real microstructure of DP590 steel to capture the mechanical behavior and fracture mode.The failure mode of the dual-phase(DP)steels,mainly resulting from microstructure-level inhomogeneity and initial geometrical imperfection,was predicted using the plastic strain localization theory.In addition,dog-bone-type tensile test specimens with different edge qualities were prepared and the deformation processes were recorded using a digital image correlation system.When the steel exhibited no initial geometrical imperfection,void initiation was triggered by decohesion between martensite and ferrite which was predicted based on the severe strain concentration,or tensile stress in areas where stress triaxiality and strain values were high.Final failure was caused by shear localization in the vicinity.Moreover,the initial geometrical imperfections severely affected the overall ductility and failure mode of the DP590steel.When initial geometrical imperfections were deeply ingrained,an incipient crack began at the site of initial geometrical imperfection,and then caused progressive damage throughout the microstructure,from the area of shear localization to the final fracture.Overall,the depth of the geometrical imperfection was the critical factor in determining whether internal decohesion or a local crack plays a dominant role. 展开更多
关键词 representative volume element dual-phasedp steel geometrical imperfection failure mode
原文传递
相同成分DP钢和TRIP钢部分力学性能的比较 被引量:26
6
作者 张继诚 符仁钰 +1 位作者 张梅 李麟 《热加工工艺》 CSCD 北大核心 2006年第22期13-16,共4页
对同一种钢板进行不同热处理分别制成具有相同铁素体含量的双相钢(DP钢)和相变诱发塑性变形钢(TRIP钢),并对其部分力学性能进行对比。比较发现,铁素体基体上不同的第二相使得材料力学性能产生巨大差异:马氏体使DP钢具有很高的抗拉强度,... 对同一种钢板进行不同热处理分别制成具有相同铁素体含量的双相钢(DP钢)和相变诱发塑性变形钢(TRIP钢),并对其部分力学性能进行对比。比较发现,铁素体基体上不同的第二相使得材料力学性能产生巨大差异:马氏体使DP钢具有很高的抗拉强度,残余奥氏体则赋予TRIP钢优良的伸长率;DP钢拥有更加优良的加工硬化能力,TRIP钢则具有较为理想的烘烤硬化能力。试验还表明,考察DP钢和TRIP钢的烘烤硬化能力时,除柯氏气团外,内应力的消除也应该考虑其中。 展开更多
关键词 dp TRIP钢 力学性能 加工硬化 烘烤硬化
下载PDF
Mo对双相钢过冷奥氏体连续冷却转变的影响 被引量:2
7
作者 罗扬 孙力 +5 位作者 熊自柳 史远 谷秀锐 白丽娟 董伊康 王健 《河北冶金》 2021年第5期8-12,76,共6页
Mo是1000 MPa级高强双相钢常用的合金元素。为了考察Mo元素对双相钢过冷奥氏体连续冷却转变的影响规律,利用光学显微镜和淬火膨胀仪,分别对不同Mo含量的含硼及含铬双相钢的静态过冷奥氏体连续冷却转变曲线(静态CCT曲线)进行了测定和比... Mo是1000 MPa级高强双相钢常用的合金元素。为了考察Mo元素对双相钢过冷奥氏体连续冷却转变的影响规律,利用光学显微镜和淬火膨胀仪,分别对不同Mo含量的含硼及含铬双相钢的静态过冷奥氏体连续冷却转变曲线(静态CCT曲线)进行了测定和比较。结果表明,Mo元素能够缩小过冷奥氏体的高温转变区域,并使高温转变和中温转变区域分离;同时,可以缩小贝氏体转变区域,并在一定程度上抑制贝氏体转变,从而提高淬透性。 展开更多
关键词 双相钢 过冷奥氏体 连续冷却转变 MO 淬透性
下载PDF
1000 MPa级冷轧双相钢氢致延迟开裂性能研究
8
作者 谢春乾 潘丽梅 +1 位作者 韩赟 刘华赛 《汽车工艺与材料》 2022年第8期53-56,共4页
采用电化学充氢、慢拉伸试验、热脱附氢检测装置(Thermal Desorption Spectroscopy,TDS)分析以及扫描电镜(Scanning Electron Microscope,SEM)方法对汽车用1000 MPa级别双相钢(DP980)的氢致延迟开裂行为进行研究。结果发现,DP980组织结... 采用电化学充氢、慢拉伸试验、热脱附氢检测装置(Thermal Desorption Spectroscopy,TDS)分析以及扫描电镜(Scanning Electron Microscope,SEM)方法对汽车用1000 MPa级别双相钢(DP980)的氢致延迟开裂行为进行研究。结果发现,DP980组织结构为铁素体、马氏体双相组织,同时在基体中含有大量NbTi析出相。随着充氢电流密度从0 mA/cm^(2)增加到16 mA/cm^(2),试样内部氢含量从0.68×10^(-6)mg/kg提高至2.10×10^(-6)mg/kg,氢致延迟断裂敏感系数由3.1%增加至5.4%。采用扫描对断口进行分析,断口状态呈现韧窝状,不具有显著的氢脆敏感性。可以看出,DP980随氢含量增加氢脆敏感性增加。 展开更多
关键词 双相钢 延迟开裂 析出相
下载PDF
边部冲裁对双相钢拉伸性能影响的实验研究 被引量:1
9
作者 郑欢 吴彦骏 +3 位作者 刁可山 庄新村 陈劼实 赵震 《上海交通大学学报》 EI CAS CSCD 北大核心 2014年第3期405-411,共7页
为研究边部冲裁对双相钢(DP590、DP780和DP980)拉伸性能的影响,采用冲裁和线切割2种方法制备实验试样.基于MTS793材料试验机,使用非接触式视频应变测量方法,在常温下完成静拉伸实验.通过材料的力学性能曲线,分析原始标距对拉伸性能的影... 为研究边部冲裁对双相钢(DP590、DP780和DP980)拉伸性能的影响,采用冲裁和线切割2种方法制备实验试样.基于MTS793材料试验机,使用非接触式视频应变测量方法,在常温下完成静拉伸实验.通过材料的力学性能曲线,分析原始标距对拉伸性能的影响以及不同断面质量下拉伸试样的力学性能响应、颈缩过程与断口形貌.结果表明:原始标距减小,基本不影响屈服强度、抗拉强度和最大力非比例伸长率,而断裂总伸长率显著增大;冲裁试样与线切割试样在拉伸颈缩段存在较大差别,断裂总伸长率低于线切割试样,且随着冲裁间隙的增大而减小;DP590和DP780冲裁试样在非均匀颈缩和横向裂纹出现后,呈现折线状断口,而DP980冲裁试样则与线切割试样的剪切滑移型断口类似,颈缩时产生显著的剪切带. 展开更多
关键词 双相钢 冲裁 拉伸 原始标距 颈缩
下载PDF
上一页 1 下一页 到第