Micro-amount terephthalic acid and 4-carboxybenzaldehyde in p-toluic acids were determined by a reversed-phase ion suppression chromatography.The separation was carried out on a C18column(4.6mm i.d.×150mm)with ...Micro-amount terephthalic acid and 4-carboxybenzaldehyde in p-toluic acids were determined by a reversed-phase ion suppression chromatography.The separation was carried out on a C18column(4.6mm i.d.×150mm)with methanol-water(70∶30)as the mobile phase at a flow rate of 0.8ml/min and with H3PO4 as an inhibitor.The detection wavelength was 240 nm.The relative standard deviation of terephthalic acid and 4-carboxybenzaldehyde are less than 3% and 2%,respectively.The average recoveries were 102.9% and 103.2%,respectively.The detection limit were 0.25 ng and 0.45 ng,respectively.展开更多
研究了用二甲苯浸出-焙烧-硫酸浸出杂质-氰化浸出银工艺从湿法炼锌渣中回收硫和银。试验结果表明:在反应温度95℃、反应时间15 min、液固体积质量比5∶1条件下用二甲苯浸出,硫浸出率为96.40%;分硫渣中加入1%氢氧化钠,在630℃下焙...研究了用二甲苯浸出-焙烧-硫酸浸出杂质-氰化浸出银工艺从湿法炼锌渣中回收硫和银。试验结果表明:在反应温度95℃、反应时间15 min、液固体积质量比5∶1条件下用二甲苯浸出,硫浸出率为96.40%;分硫渣中加入1%氢氧化钠,在630℃下焙烧2 h ,然后用硫酸浸出锌、铁等杂质,控制液固体积质量比为4∶1,pH为1.0,反应温度为95℃,反应时间为3h;之后对硫酸浸出渣氰化浸出银,体系pH控制在9.5~11.5之间,液固体积质量比为3∶1,氰化钠质量浓度2.0g/L,浸出时间24h,银回收率为78.5%。展开更多
文摘Micro-amount terephthalic acid and 4-carboxybenzaldehyde in p-toluic acids were determined by a reversed-phase ion suppression chromatography.The separation was carried out on a C18column(4.6mm i.d.×150mm)with methanol-water(70∶30)as the mobile phase at a flow rate of 0.8ml/min and with H3PO4 as an inhibitor.The detection wavelength was 240 nm.The relative standard deviation of terephthalic acid and 4-carboxybenzaldehyde are less than 3% and 2%,respectively.The average recoveries were 102.9% and 103.2%,respectively.The detection limit were 0.25 ng and 0.45 ng,respectively.
文摘研究了用二甲苯浸出-焙烧-硫酸浸出杂质-氰化浸出银工艺从湿法炼锌渣中回收硫和银。试验结果表明:在反应温度95℃、反应时间15 min、液固体积质量比5∶1条件下用二甲苯浸出,硫浸出率为96.40%;分硫渣中加入1%氢氧化钠,在630℃下焙烧2 h ,然后用硫酸浸出锌、铁等杂质,控制液固体积质量比为4∶1,pH为1.0,反应温度为95℃,反应时间为3h;之后对硫酸浸出渣氰化浸出银,体系pH控制在9.5~11.5之间,液固体积质量比为3∶1,氰化钠质量浓度2.0g/L,浸出时间24h,银回收率为78.5%。